The present invention relates to a low noise asphalt mixture and a method for producing and mixing the asphalt mixture. The present invention relates to a low noise asphalt mixture comprising 5-10% pure asphalt, 2-7% waste tire rubber powder, 3-8% A mixture prepared by mixing one mixture and the balance% of aggregate at a temperature of 180 ° C or higher; A first step of mixing the asphalt mixture in an asphalt mixing plant; A second step of transferring the mixture mixed in the first step to the site at a speed of 40 km; The mixture transferred to the second step is mixed with 80 to 84% of asphalt materials having an invasion degree of about 35 to 50 to 16 to 20% of a mixed solution of a polypropylene polymer, a thermoplastic resin, a pohutland resin, A third step of placing the manufactured waterproof body at 150 DEG C or higher; And a fourth step of compaction of the third stage with the vibration tire rollers when the third step is completed.
机译:低噪声沥青混合料及其生产和混合方法技术领域本发明涉及一种低噪声沥青混合料及其生产和混合的方法。本发明涉及一种低噪音的沥青混合物,其包含5-10%的纯沥青,2-7%的废轮胎橡胶粉,3-8%的混合物,该混合物通过在180°C的温度下将一种混合物与余量的骨料混合而制备。 C或更高;在沥青混合设备中混合沥青混合物的第一步;第二步是将第一步中混合的混合物以40 km的速度转移到现场;将转移到第二步的混合物与80-84%沥青质材料混合,该沥青材料的入侵度约为35-50-50-16%20%的聚丙烯聚合物,热塑性树脂,pohutland树脂,将制造的防水体放置在150℃或更高的步骤;第三步完成时,第三步是用振动轮胎辊压实第四步。

著录项

  • 公开/公告号KR19990007510A

    专利类型

  • 公开/公告日1999-01-25

    原文格式PDF

  • 申请/专利权人 김현준;

    申请/专利号KR19980029277

  • 发明设计人 김현준;

    申请日1998-07-21

  • 分类号C04B24/36;

  • 国家 KR

  • 入库时间 2022-08-22 02:18:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号