Plasma transferred arc powder weld deposition on easily oxidized materials is carried out using a weld filler material of a CuNi alloy with certain alloy additions. In the process for coating of easily oxidized materials by plasma transferred arc powder weld deposition using d.c. or d.c.-superimposed a.c. by the method described in DE 19626941.5, the weld filler material comprises a CuNi alloy with additions of (by wt.) (a) less than 10% Fe, less than 5% Cr, less than 4% B, less than 4% Si and about 1.5% C, the mixing ratio with the parent material being more than 40 vol.%, or (b) less than 10% Mo, Mn, Co, Ti, Ta, Zr and Mg and less than 2% P and N. Preferred Features: The resulting deposit comprises a metallic matrix containing (by wt.) 30-70% Al, 42-21% Cu, 18-9% Ni, 6-2% Fe, 4-0.5% Cr, 1.8-0.5% Si, less than 2% B and less than 10% others.
机译:等离子转移电弧粉末焊接沉积在易氧化的材料上是通过使用CuNi合金的焊接填充材料并添加某些合金来进行的。在使用dc的等离子转移电弧粉末焊接沉积方法涂覆易氧化材料的过程中。或直流叠加的交流电通过DE 19626941.5中描述的方法,焊缝填充材料包括CuNi合金,其添加(以重量计)(a)小于10%的Fe,小于5%的Cr,小于4%的B,小于4%的Si大约1.5%的C,与母体材料的混合比例大于40%(体积),或(b)小于10%的Mo,Mn,Co,Ti,Ta,Zr和Mg,小于2%的P和N优选特征:所得沉积物包含金属基质,该金属基质包含(以重量计)30-70%Al,42-21%Cu,18-9%Ni,6-2%Fe,4-0.5%Cr,1.8-0.5 %的Si,小于2%的B和小于10%的其他。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号