首页> 外国专利> Solid electrolyte for sodium-sulfur battery and method for producing sodium-sulfur battery using the same

Solid electrolyte for sodium-sulfur battery and method for producing sodium-sulfur battery using the same

机译:钠硫电池用固体电解质及使用该固体电解质的钠硫电池的制造方法

摘要

PURPOSE:To suppress the deterioration of beta-alumina-based ceramics due to humidity absorption by coating the beta-alumina-based ceramics with a water repelling material, granulating the ceramics to have prescribed particle size, and then firing the resulting ceramics. CONSTITUTION:A synthetic powder of beta''-alumina, a beta-alumina-based ceramic consisting of beta-alumina, or a ceramic containing both ceramics is coated with a water repelling material. The resulting powder is granulated into 30-100mum particle size and the granulated powder is molded and then sintered. As a result, at the time of production of solid electrolytes, deterioration and size alteration due to humidity absorption before sintering and damage and crack formation attributed to them at the time of sintering are suppressed and formability is improved. a sodium-sulfur battery having the solid electrolyte prepared in that way surely has high reliability. Furthermore, since coating with the water repelling material is done, materials containing water as a main component may be selected as a binder and a solvent at the time of granulation and thus there is a wide option to select binders and solvents.
机译:目的:为抑制β-氧化铝基陶瓷因吸湿而导致的变质,方法是在该β-氧化铝基陶瓷上涂上拒水材料,将陶瓷造粒至规定的粒径,然后烧制所得陶瓷。组成:β”-氧化铝的合成粉末,由β-氧化铝组成的基于β-氧化铝的陶瓷或包含两种陶瓷的陶瓷均涂有拒水材料。将所得粉末造粒为30-100μm的粒度,并将造粒的粉末成型然后烧结。结果,在制造固体电解质时,抑制了由于烧结前的吸湿引起的劣化和尺寸变化以及在烧结时归因于它们的损坏和裂纹形成,并且改善了可成形性。具有这样制备的固体电解质的钠硫电池肯定具有高可靠性。此外,由于已经完成了用拒水材料的涂覆,因此在造粒时可以选择以水为主要成分的材料作为粘合剂和溶剂,因此,存在选择粘合剂和溶剂的广泛选择。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号