摘要

PROBLEM TO BE SOLVED: To restrain the surface defect and the internal defect and to improve the yield of a cast slab while eliminating grind-cleaning and developing scrapping by specifying a specified ration or more of the whole cross section on a cast slab so as to form fine solidified structure. ;SOLUTION: An equi-axed crystal of the case slab satisfies the formula at ≥60% of the whole cross sectional area in the cast slab (in the formula, X: distance (mm) from the surface of the cast slab, D: diameter (mm) of the equi-axed crystal at the position of X from the surface of the cast slab). It is desirable to fill the equi-axed crystal in the cast slab excellent in a rolling characteristic in the whole cross section of the cast slab and be a steel material having the max. equi-axed crystal diameter in the cast slab within 3 times of the average equi-axed crystal diameter. In this way, the growth of columnar crystal on the surface layer of the cast slab is restrained and the fine equi-axed crystal is formed in the inner part. The surface defect of crack, recessed flow, etc., generated from micro-segregating part as the starting point at the cooling time and at the solidifying time, can be restrained. Further, the micro-segregation at the boundary part is reduced and the internal crack caused by the shrinkage, the bulging of the cast slab, the straightening of bending-back, etc., and the internal defect of the center segregation, etc., caused by the cavity and the fluid of unsolidified steel, are prevented.;COPYRIGHT: (C)2000,JPO
机译:解决的问题:通过在铸坯上指定整个横截面的指定比例或更多,以消除铸坯的表面缺陷和内部缺陷,并提高铸坯的产量,同时消除研磨清洁和产生的报废现象,从而形成优良的凝固组织。 ;解决方案:壳体平板的等轴晶体在铸坯总横截面的≥60%时满足公式(公式中,X:距铸坯表面的距离(mm),D:从铸坯表面到X位置的等轴晶体的直径(mm))。理想的是在铸坯的整个横截面中将具有优异的轧制特性的等轴晶体填充在铸坯中,并且该铸坯具有最大的塑性。铸坯的等轴晶体直径在平均等轴晶体直径的3倍以内。这样,抑制了柱状晶体在铸坯表面层上的生长,并且在内部形成了细等轴晶体。可以抑制在冷却时和固化时由微偏析部作为起点产生的裂纹,凹陷流等的表面缺陷。此外,减少了边界部分的微偏析,并且由收缩,铸坯的鼓出,向后弯曲的拉直等,以及中心偏析的内部缺陷等引起的内部裂纹减少,防止因空洞和未凝固的钢液引起的腐蚀。;版权:(C)2000,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号