PROBLEM TO BE SOLVED: To provide Ni refined steel excellent in tempering brittleness resistance and hydrogen brittleness resistance. ;SOLUTION: In steel contg., as fundamental components, by weight, 0.05 to 0.4% C, 0.02 to 0.6% Si, 0.02 to 2.0% Mn, 0.02 to 3.0% Mo, 0.01 to 5.0% Cr, 3.0 to 10.0% Ni, 0.001 to 0.03% P, 0.0005 to 0.03% S and 0.001 to 0.015% N, and the balance Fe with inevitable impurities, the content of Al in the old austenitic grain boundaries is controlled to ≥0.6%, or the content of {Al-(Si+Mn+Cr)} in the grain boundaries is controlled to the value of ≥3%, or the content of (Si+Mn+Cr) in the grain boundaries is controlled to ≤3.5%. If required, one or ≥ two kinds among Cu, Nb, V, Ti and B are moreover incorporated therein.;COPYRIGHT: (C)2000,JPO
机译:解决的问题:提供耐回火脆性和耐氢脆性优异的镍精炼钢。 ;解决方案:在钢中,以重量计,基本成分为0.05至0.4%C,0.02至0.6%Si,0.02至2.0%Mn,0.02至3.0%Mo,0.01至5.0%Cr,3.0至10.0%Ni ,0.001到0.03%的P,0.0005到0.03%的S和0.001到0.015%的N,以及带有不可避免杂质的余量Fe,旧奥氏体晶界中的Al含量控制在≥0.6%,或{Al的含量将晶界中的-(Si + Mn + Cr)}控制为≥3%的值,或者将晶界中的(Si + Mn + Cr)的含量控制为≤3.5%。如果需要的话,还可以掺入Cu,Nb,V,Ti和B中的一种或两种以上。版权所有:(C)2000,JPO

著录项

  • 公开/公告号JP2000212705A

    专利类型

  • 公开/公告日2000-08-02

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CORP;

    申请/专利号JP19990013501

  • 申请日1999-01-21

  • 分类号C22C38/00;C21D6/00;C22C38/58;

  • 国家 JP

  • 入库时间 2022-08-22 01:59:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号