首页> 外国专利> Process for the treatment of steel slag and iron substrates to obtain crude iron and environmentally compatible slag

Process for the treatment of steel slag and iron substrates to obtain crude iron and environmentally compatible slag

机译:用于处理钢渣和铁底材以获得粗铁和与环境相容的炉渣的方法

摘要

Invention Patent: B "PROCESS FOR THE TREATMENT OF STEEL SLAG AND IRON SUBSTRATES FOR THE OBTAINING OF CRUDE IRON AND SLOTS COMPATIBLE WITH THE ENVIRONMENT" D. With a process for the treatment of steel slag and iron substrates, such as, for example, slag from converter, slag from converter, fine ores, powders from the preparation of steel, scales from roller mills to obtain crude iron and environmentally compatible slag, the proportion by volume of molten slag with respect to iron bath is chosen greater than 0.5 to 1, preferably 0.8: 1 to 1.5: 1, and SiO ~ 2 ~ substrates are added to the slag, such as, for example, foundry sands, metallurgical sands and / or fine ores, to adjust a slag basicity (CaO / SiO ~ 2 ~) between 1 , 0 and 1.8 preferably between 1.2 and 1.8, with an Al ~ 2 ~ O ~ 3 ~ content between 10 and 25% by weight, with respect to slag. In this case, air and coal jets are inflated, possibly with inert gas, especially with nitrogen and in addition, eventually, oxygen or hot air is permeated by the iron bath.
机译:发明专利:“用于获得粗铁和与环境相适应的狭缝的钢渣和铁基体的处理方法” 。采用一种处理钢渣和铁基质的方法,例如转炉产生的炉渣,转炉产生的炉渣,细矿,制备钢的粉末,辊磨机产生的氧化皮,以获得粗铁和与环境相容的炉渣,选择熔渣相对于铁水的体积比例大于0.5:1,优选为0.8:1至1.5:1,并且将SiO〜2〜基质添加到炉渣中,例如铸造砂,冶金砂和/或细矿,以将矿渣碱度(CaO / SiO〜2〜)调节在1,0至1.8之间,最好在1.2至1.8之间,其中Al〜2〜O〜3〜的含量在10%至25%之间重量,相对于炉渣。在这种情况下,可能会用惰性气体(尤其是氮气)对空气和煤炭喷射器进行充气,此外,最终,铁熔池会渗透氧气或热空气。

著录项

  • 公开/公告号BR9806267A

    专利类型

  • 公开/公告日2000-04-04

    原文格式PDF

  • 申请/专利权人 HOLDERBANK FINANCIERE GLARUS AG.;

    申请/专利号BR19989806267

  • 发明设计人 ALFRED EDLINGER;

    申请日1998-09-08

  • 分类号C21C5/36;C22B7/04;

  • 国家 BR

  • 入库时间 2022-08-22 01:57:15