Process for producing a precipitated calcium carbonate aragonu00ectico finely and roughly mou00ecdo and a product of aragonita, and product of aragonita ".Precipitated calcium carbonate aragonu00edtico, finely granular, is produced on a commercial scale by seeding with a precipitated calcium carbonate aragonu00edtico roughly granulated.The material of the seeding roughly granules is produced by interrupting if, after the production of 0.1 to 0.6 g / 1 / min of calcium carbonate.The supply of carbon dioxide into the lime mud alive at the beginning of the reaction, to allow subsequ00b3ente nucleation of crystals and, subsequently,Continue the supply of carbon dioxide in the rates of reaction of 0,1 g / 1 min to 0.6 g / 1 min.This material for seeding roughly granules has a surface area of Blaine can be smaller than 30.000 cm ^ 2 ^ / g, the solids are 35 to 70 percent by weight aragonita, and is added in subsequ00b3entes batching as a mud to about 1 percent by weight.Based on the total weight of the mud of the material to be sown.For the batching sown, carbonation is carried out in the rates of reaction of up to 1.8 g / 1 min on a commercial scale, resulting in the product aragonitu00edco finely granulated.This product with its end does not need to ground, is solid in which the percentage by weight of aragonita is greater than 90, has an average particle size between 0.3 to about 0.5 microns.A particle size distribution in which about 60 to 70 per cent by weight have the equivalent spherical diameter smaller than 0.5 micro.And a surface area of Blaine, who can be more than 35000 cm ^ 2 ^ / g.
机译:精细地和粗略地制造沉淀碳酸钙阿拉贡的方法,以及阿拉贡塔的产物和阿拉贡塔的产物。沉淀的碳酸钙阿拉贡细粒,通过将沉淀的种子播种而以商业规模生产。碳酸钙氩粗粒状。如果在生成0.1至0.6克/分钟/分钟的碳酸钙后中断生产,则粗粒状种子的材料将被中断。反应开始时,为了使晶体随后成核,随后以0.1 g // 1分钟至0.6 g // 1分钟的反应速率继续供应二氧化碳。粗粒的Blaine表面积可小于30.000 cm ^ 2 ^ / g,固体含量为35%至70%(重量)的阿拉贡(aragonita),并作为泥浆分批添加至约1%(重量)。基于 对于要播种的配料,以商业规模以高达1.8 g / min的反应速率进行碳酸化,从而使产品aragonitededco细粒化该产品的末端无需研磨,是一种固体,其中Aragonita的重量百分比大于90,其平均粒径在0.3到约0.5微米之间。粒径分布在每颗中约60到70按重量计,当量球形直径小于0.5微米,而布莱恩的表面积则可以超过35000 cm ^ 2 ^ / g。

著录项

  • 公开/公告号BR9809130A

    专利类型

  • 公开/公告日2000-08-01

    原文格式PDF

  • 申请/专利权人 ECC INTERNATIONAL INC;

    申请/专利号BR19989809130

  • 发明设计人 STEVEN M. FORTIER;BRUCE JACKSON;

    申请日1998-05-08

  • 分类号C01F11/00;

  • 国家 BR

  • 入库时间 2022-08-22 01:57:13

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号