AQUEOUS COATING MEDIUM, METHOD OF OBTAINING SAME AND APPLICATION THEREOF IN PRODUCTION OF STOVING LACQUERS AND OF COATING DRYING AS RESULT OF EXPOSURE TO PHYSICAL FACTORS

机译:物理因素导致的水性漆介质,同样的获得方法及其在生产漆和干燥漆中的应用

摘要

The use of an aqueous dispersion of a polyol component, comprising 20-60 wt.% unsaturated polyester polyol and 40-80 wt.% polyacrylate, and 1-70 wt.% (with respect to total solids) of a blocked aliphatic polyisocyanate component for light-stable, elastic, physically fast-drying coatings in series lacquering of cars is claimed. The use of an aqueous dispersion of (A) a polyol component and (B) a polyisocyanate component for light-stable, elastic, physically fast-drying coatings in series lacquering of cars is claimed. The polyol component comprises 20-60 wt.% polyester component (AI) with 10-60 wt.% units derived from 8-30 carbon (C) aliphatic (un)saturated monocarboxylic acid(s) and 0.4-5 wt.% units derived from 3-8 C alpha , beta -unsaturated mono- or dicarboxylic acid(s) or anhydride(s) capable of free radical polymerization and 40-80 wt.% polyacrylate component (AII). The polyisocyanate component (B) comprises blocked aliphatic polyisocyanate(s) and is used in an amount of 1-70 wt.% with respect to total solids in the dispersion.
机译:多元醇组分的水分散体的用途,所述多元醇组分包含20-60重量%的不饱和聚酯多元醇和40-80重量%的聚丙烯酸酯和1-70重量%(相对于总固体)的封端的脂族多异氰酸酯组分要求对汽车进行系列上光的光稳定,弹性,物理上快干的涂料。要求将(A)多元醇组分和(B)多异氰酸酯组分的水分散体用于汽车的连续涂漆的光稳定的,弹性的,物理上快干的涂料中。多元醇组分包含20-60重量%的聚酯组分(AI),其具有10-60重量%的单元,其衍生自8-30个碳(C)脂族(不饱和)单羧酸和0.4-5重量%的单元。衍生自能够进行自由基聚合的3-8 Cα,β-不饱和一元或二元羧酸或酸酐和40-80 wt%的聚丙烯酸酯组分(AII)。多异氰酸酯组分(B)包含嵌段的脂族多异氰酸酯,并且相对于分散体中的总固体以1-70重量%的量使用。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号