The present invention concerns a PREPARATION OF A THIN FILM shrinkable BIOORIENTADA PROCESS PROCESS IN PLANE polyethylene-based linear low density CHARACTERIZED IN THAT: -is BEYOND THE HEAT melting temperature and extruded, alone or in mixture with a homopolymer of ethylene or a copolymer of ethylene and of an alpha-olefin comonomer in (SUB {9}) A (SUB {18}) density between 0.89 and 0.94, - strained and cooled A FITTING THE anneal temperature extruded film; - Stretches A FIRST TIME IN THE MEANING OF LAMAQUINA THIS MOVIE TO PROPER TEMPERATURE from 3 to 7 times the initial size of the undrawn film - Stretches A SECOND TIME IN THE SENSE PENETRATED THROUGH THIS unstretched film at temperature, Stretches UNATERCERA time in the machine direction MOVIE TO PROPER TEMPERATURE BIORRIENTADA between 1.01 and 3 times the dimension after the first sTRETCHED, cooled BIORRIENTADA FILM OBTAINED AT ROOM TEMPERATURE. ALSO it REFERS TO A FILM ULTRA MONOCAPA particularly the process.
机译:本发明涉及一种在平面的基于聚乙烯的线性低密度的薄膜可收缩的生物材料中的制备方法,其特征在于:-比热熔融温度高并且单独或与乙烯的均聚物或乙烯的共聚物混合挤出。 (a)(SUB {9})的α-烯烃共聚单体(SUB {18})密度在0.89至0.94之间;-应变并冷却。 -在拉玛奎那影片的意义上将其第一次拉伸至合适温度,是未拉伸膜的初始尺寸的3到7倍-在感官上穿透第二次穿透该未拉伸膜的温度,在机器方向上拉伸未拉伸时间在室温下获得第一次拉伸,冷却的BIORRIENTADA膜后,将适当的温度移动到BIORRIENTADA的尺寸的1.01到3倍之间。此外,它还特别适用于电影超单声道电影。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号