摘要

The present invention relates to polymer electrolyte compositions comprising polyvinylchloride / poly (methylmethacrylate) (PVC / PMMA) blends, ethylene carbonate, propylene carbonate and lithium salts, and to methods for the convenient preparation of electrical polymer electrolyte compositions. According to the present invention, the polymer electrolyte composition including the PVC / PMMA blend is 18.0 to 45.0 wt% of PVC / PMMA blend, 30.0 to 45.0 wt% of ethylene carbonate, mixed with 90 to 10 wt% of PVC and 10 to 90 wt% of PMMA, Propylene carbonate 20.0 to 32.0 and lithium salt 2.0 to 7.0% by weight. The polymer electrolyte composition of the present invention is prepared by mixing PVC / PMMA blend, ethylene carbonate, propylene carbonate, and lithium salt mixed with PVC and PMMA, dissolving in a nonpolar solvent, casting and drying in a mold. The polymer electrolyte composition of the present invention is excellent in mechanical properties and ionic conductivity, as well as interfacial adhesion, can be easily prepared by mixing the components of the composition and can be prepared at a low cost because it uses a general-purpose polymer.
机译:本发明涉及包含聚氯乙烯/聚(甲基丙烯酸甲酯)(PVC / PMMA)共混物,碳酸亚乙酯,碳酸亚丙酯和锂盐的聚合物电解质组合物,以及用于方便地制备电聚合物电解质组合物的方法。根据本发明,包括PVC / PMMA共混物的聚合物电解质组合物为PVC / PMMA共混物的18.0至45.0重量%,碳酸亚乙酯的30.0至45.0重量%,与90至10重量%的PVC和10至90的重量比混合。重量%的PMMA,碳酸亚丙酯20.0至32.0和锂盐2.0至7.0重量%。通过将PVC / PMMA共混物,碳酸亚乙酯,碳酸亚丙酯和锂盐与PVC和PMMA混合,将其溶于非极性溶剂中,浇铸并在模具中干燥,来制备本发明的聚合物电解质组合物。本发明的高分子电解质组合物的机械特性,离子传导性以及界面密合性优异,通过使用通用的聚合物,可以容易地混合组合物的成分来制造,并且可以低成本地制造。 。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号