PURPOSE: Provided is a compressed complex gunpowder composition of which charging density is increased and which is insensitive to an external shock. CONSTITUTION: The compressed complex gun powder comprises: (i) 90-96 wt.% of raw material powder(H.M.X); (ii) 1-3 wt.% of acrylate elastic copolymer(HyTemp-4404) as a crosslinking monomer having reactive hydroxy group; and (iii) 3-9 wt.% of D.O.A. The method comprises steps of: (i) dissolving 15-20 wt.% of the acrylate elastic copolymer(HyTemp-4404) in ethyl acetate at a temperature of 50-60 deg.C to prepare a liquid polymer solution; (ii) dispersing 8.0-11.0 wt.% of H.M.X in water to prepare a slurry solution; and (iii) after injecting the polymer solution into the slurry solution at a temperature of 60-70 deg.C to form a granular body, distilling the granular body.
机译:目的:提供一种压缩复合火药组合物,其装填密度增加并且对外部冲击不敏感。组成:压缩复合枪粉包括:(i)90-96 wt。%的原料粉末(H.M.X); (ii)1-3 wt。%的丙烯酸酯弹性共聚物(HyTemp-4404)作为具有反应性羟基的交联单体; (iii)D.O.A.的3-9 wt。%该方法包括以下步骤:(i)在50-60℃的温度下将15-20重量%的丙烯酸酯弹性共聚物(HyTemp-4404)溶解在乙酸乙酯中以制备液体聚合物溶液; (ii)将8.0.11.0重量%的H.M.X分散在水中以制备浆液; (iii)在60-70℃的温度下将聚合物溶液注入淤浆溶液中以形成粒状体,然后蒸馏该粒状体。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号