(57) to precipitate zirconium hydroxide pH value of 4 to 10 to be achieved using a base from [Abstract] zirconium salt solution, aqueous solutions of salts and possibly other copper zirconium hydroxide suspension was added to precipitate the pH value of 8 to 14 until is achieved, the hydroxide of metal contained in the salt of the other, was obtained and in some cases copper hydroxide by the addition of other bases It is the suspension was filtered, washed, dried, calcined so as to contact the 2 to 4 hours in air at 450~600 ℃, is reduced 2-4 hours in a stream of hydrogen at 200~250 ℃ finally by containing other metals can be produced, in some cases zirconium, copper, metal described at that time, is reduced are precipitated as hydroxides, washed, dried, and and calcined, catalysts for the dehydrogenation to oxy-carboxylic acid ethylene glycol or dehydrogenation of (derivative) to the amino acid amino alcohol.
机译:(57)使用[盐]锆盐溶液中的碱沉淀出氢氧化锆的pH值为4至10,加入盐的水溶液和可能的其他氢氧化铜锆悬浮液以沉淀pH值为8至14,直至实现该反应,获得另一种盐中所含的金属的氢氧化物,在某些情况下,通过添加其他碱来获得氢氧化铜。将悬浮液过滤,洗涤,干燥,煅烧使其接触2至4小时在450〜600℃的空气中,在200〜250℃的氢气流中还原2-4小时,最终可以通过包含其他金属来生产,在某些情况下,锆,铜,当时描述的金属被还原沉淀作为氢氧化物,经过洗涤,干燥和煅烧后,可用于脱氢成羟基羧酸乙二醇或将(衍生物)脱氢成氨基酸氨基醇的催化剂。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号