Reform manner null of Al sintering machine

机译:铝烧结机的改造方式无效

摘要

PURPOSE: To stably sinter without damaging a die and obtain the stable dimension after sintered. ;CONSTITUTION: In correcting of Al base sintered machine part of a real density ratio after sintering being 80 to 100%, plural numbers of recessing parts 12a, 12c, 12e and projecting parts 12b, 12d, 12f are installed at least on one side face among the internal face of a die 12 or the external face of a core rod. In the recessing parts 12a, 12c, 12e, the coining stock with an body to be corrected is made under than 0. In the projecting parts 12b, 12d, 12f, the coining stock c is 10 to 100μm. When the body 11 to be corrected is reciprocated at least by one time on the projecting parts 12b, 12d in the up and down axial direction of the die, the corrected body with a prescribed dimension is obtained. Without damaging the die, the coining stock c can be made largely. Without relating to the dispersion of dimension of the body 11 to be corrected, the coining stock c is stabilized in positive.;COPYRIGHT: (C)1996,JPO
机译:用途:稳定地烧结而不损坏模具,并在烧结后获得稳定的尺寸。 ;组成:在校正烧结后实际密度比为80%至100%的Al基烧结机零件时,至少在一个侧面上安装了多个凹槽部12a,12c,12e和凸出部12b,12d,12f。在模具12的内表面或芯棒的外表面之间。在凹进部分12a,12c,12e中,具有要校正的物体的铸币被制成小于0。在突出部分12b,12d,12f中,铸币c为10至100μm。当待校正的主体11在模具的上下轴向上在突出部12b,12d上至少往复运动一次时,获得具有预定尺寸的已校正的主体。在不损坏模具的情况下,可以大量制造精铸料c。与要校正的主体11的尺寸分散无关,精铸料c稳定在正数。;版权所有:(C)1996,日本特许厅

著录项

  • 公开/公告号JP3170781B2

    专利类型

  • 公开/公告日2001-05-28

    原文格式PDF

  • 申请/专利权人 三菱マテリアル株式会社;

    申请/专利号JP19950025354

  • 发明设计人 桑原 裕司;細野 克明;

    申请日1995-02-14

  • 分类号B21D3/10;B22F3/24;B30B11/02;

  • 国家 JP

  • 入库时间 2022-08-22 01:33:40

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号