AQUEOUS COATING COMPOSITION AND CORROSION-RESISTANT METALLIC PLATE USING THE SAME AND METALLIC TANK FOR COMBUSTIBLE ORGANIC SOLVENT

机译:使用与金属罐相同的金属罐作为可燃有机溶剂的水性涂料组合物和耐腐蚀金属板

摘要

PROBLEM TO BE SOLVED: To obtain the subject curable composition capable of providing organic composite steel plates excellent in corrosion resistance and processability and designed for toxic substance-free gasoline tanks by including colloidal silica, at least one phosphoric salt-based compound and an aqueous resin. ;SOLUTION: This curable composition is obtained by including (A) colloidal silica, (B) at least one phosphoric salt-based compound and (C) an aqueous resin. The particle diameter of the component A is preferably ≤20 nm, more preferably ≤10 nm. The component B is e.g. a phosphoric acid metal salt, phosphomolybdic acid metal salt, phosphoric acid, rust-proofing pigment using them. The component C is preferably (epoxy-modified) polyester resin, polyurethane resin or the like. The compounding amount of the component A is preferably 5-100 pts.wt. based on 100 pts.wt. of the component C and that of the component B is preferably 5-100 pts.wt. The other objective metallic tank for a combustible organic solvent is provided by laminating this composition in the internal side thereof.;COPYRIGHT: (C)2001,JPO
机译:要解决的问题:通过包含胶体二氧化硅,至少一种磷酸盐基化合物和水性树脂,获得能够提供耐腐蚀性和加工性优异并且设计用于无毒汽油箱的有机复合钢板的主题可固化组合物。 。 ;解决方案:该可固化组合物是通过包含(A)胶态二氧化硅,(B)至少一种基于磷酸盐的化合物和(C)水性树脂而获得的。组分A的粒径优选为≤20nm,更优选为≤10nm。组分B是例如。使用它们的磷酸金属盐,磷钼酸金属盐,磷酸,防锈颜料。组分C优选为(环氧改性的)聚酯树脂,聚氨酯树脂等。组分A的混合量优选为5-100pts.wt。基于100pts.wt。组分C和组分B的比优选为5-100pts.wt。另一种用于可燃有机溶剂的目标金属罐是通过在其内侧层压该组合物而提供的。版权所有:(C)2001,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号