This is a belt used to make paper, which includes a resin polymer, improved elonga. The paper tape of the invention includes a transition component and a resin polymer, wherein the resin polymer shows enhanced sublimation at ambient temperature and high temperature, while maintaining resistance to gradual decline without excessive loss of resistance to pressure. In paper tape, the resin polymer of the invention can also be used for other purposes. A paper belt containing a resin polymer,said resinous polymer is arranged in a patterned frame and wherein said resinous polymer after curing has an elongation of at least about 100% and a tensile strength of at least 182.8 kg / cm2 where said elongation and Tension are measured at a temperature of 22 degrees Celsius. A papermaking belt where said belt comprises a resinous polymer,said resinous polymer is arranged in a patterned frame and wherein said resinous polymer after curing has an elongation of at least about 45% and a tensile strength of at least 49.1 kg / cm2 where said elongation and Tension are measured at a temperature of 90 degrees Celsius. A papermaking belt where said belt comprises a resinous polymer,said polymeric resin is arranged in a patterned framework and wherein said resin polymer after curing is aged for 24 hours at a temperature of approximately 140 degrees Celsius has an elongation of at least approximately 70% and a tensile strength of at least minus 907 kg / cm2 where said elongation and tension are measured at a temperature of 22 degrees Celsius.
机译:这是一种用于造纸的皮带,其中包括树脂聚合物和改进的伸长率。本发明的纸带包括过渡组分和树脂聚合物,其中该树脂聚合物在环境温度和高温下显示出增强的升华,同时保持了耐逐渐下降的能力而没有过多的耐压性损失。在纸带中,本发明的树脂聚合物也可以用于其他目的。包含树脂聚合物的纸带,所述树脂聚合物布置在图案框架中,并且其中所述固化后的树脂聚合物具有至少约100%的伸长率和至少182.8kg / cm 2的拉伸强度,其中所述伸长率和张力为在22摄氏度的温度下测量。造纸带,其中所述带包括树脂聚合物,所述树脂聚合物布置在图案框架中,并且其中所述树脂聚合物在固化后具有至少约45%的伸长率和至少49.1kg / cm 2的拉伸强度。和张力是在摄氏90度的温度下测得的。造纸带,其中所述带包括树脂聚合物,所述聚合物树脂布置在构图的框架中,并且其中所述固化后的树脂聚合物在约140摄氏度的温度下老化24小时,其伸长率至少约70%,并且拉伸强度至少为负907 kg / cm2,其中所述伸长率和张力是在22摄氏度的温度下测量的。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号