AbstractProcess for the butt welding of crosslinked polyethylene pipes (PE-X pipes)The invention relates to a method for the butt welding of crosslinked polyethylene pipes in order to utilize these pipes in industrial and underground pipeline construction.According to the invention, the pipe end faces of the PE-X pipes are spatially melted by a serrated heating element, temperature 420[err]C but 450[err]C, with a warming-up time 60 s, in such a way that enlarged and serrated pipe end faces are produced, the integral melt layers of which come into connection with one another during the joining process under a welding pressure of 0.10 to 0.40 N/mm[err] in such a way that a melt phase of these layers which is capable of entering into a connection evokes a mixing effect of the melt by means of turbulent movements at the contacting tooth flanks and a spatially distributed weld seam is produced with an enlarged binding surface.The welding pressure is maintained until the joining zone has cooled to ambient temperature, figure 2.With the butt welding method according to the invention, PE-X pipes can be connected to one another directly in a permanent and durable manner and without welding auxiliary means or an additional material.
机译:抽象交联对接工艺聚乙烯管(PE-X管)本发明涉及一种屁股的方法焊接交联聚乙烯管在工业和地下工程中利用这些管道管道建​​设。根据本发明,管端面的PE-X管道在空间上被锯齿状熔化加热元件,温度> 420°C但<450°C,带有预热时间> 60 s,以使产生锯齿状的管道端面,整体熔化它们的各层相互联系在焊接压力为0.10至0.40 N / mm [err]的熔融相为这些能够进入连接通过以下方式引起熔体的混合效果齿侧面的湍流运动然后产生一个空间分布的焊缝扩大的装订表面。保持焊接压力直到连接区域已冷却至环境温度,图2。采用对焊方法发明,PE-X管道可以相互连接直接以永久和持久的方式进行焊接辅助工具或其他材料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号