The present invention provides an electrodeposited copper foil which solves problems of electrodeposited-copper-clad laminates to which the foil has been incorporated, such as bow, twist, and poor dimensional stability, and a method of inspecting an electrodeposited copper foil so as to assure the quality of the foil. In the invention, there is employed an electrodeposited copper foil which recrystallizes by heating at low temperature during production of a copper-clad laminate employing an electrodeposited copper foil and which exhibits an elongation as high as 18% or more in an atmosphere of 180 C., wherein the maximum rate of decrease in maximum tensile strength falls within the aging time ranging from 5 to 10 minutes in a process in which tensile strength decreases as time elapses during aging in an atmosphere at 170 C., and the change in tensile strength in a knick portion shown in a tensile strength vs. aging time curve which is drawn in an x-y plane and which has a knick portion is 3 kg/mm2 or more, the x-axis representing aging time and the y-axis representing tensile strength.
机译:本发明提供一种电沉积铜箔,该电沉积铜箔解决了结合有该箔的电沉积铜覆层层压板的弯曲,扭曲和差的尺寸稳定性等问题,并且提供了一种检查电沉积铜箔的方法以确保铝箔的质量。在本发明中,使用电沉积铜箔,其在使用电沉积铜箔的覆铜层压板的生产过程中通过在低温下加热而重结晶,并且在180℃的气氛中显示出高达18%或更高的伸长率。 ,其中最大拉伸强度的最大降低速率在老化过程中在5至10分钟的范围内,在该过程中,拉伸强度随着在170°C的气氛中的老化过程中时间的流逝而降低,并且在xy平面上绘制的具有抗弯强度的抗拉强度与时效时间曲线中所示的尼克部分为3 kg / mm 2 或更高,x轴表示时效时间, y轴表示抗拉强度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号