[Summary] [challenge] is a stress relief grain size is small workability before annealing is good, the excellent non-oriented electrical steel sheet of iron loss to the crystal grains grow significantly after stress relief annealing, and its manufacturing method to provide. A by mass%, C: 0.010% or less, Mn: 0.1% for more than one. 5%, Si: 0.1% or 4% or less, Al: 0.1% or 4% or less, Si + M n + Al ≦ 5.0%, Mg: 0.0005% or more than 0.020%, or even Ca: 0.0005% or more, Mg + Ca: 0.020% or less, or REM: 0. 0,005% or more, Mg + REM: 0.020% or less, or Ca, REM 0.0005% or more, respectively, Mg + Ca + REM: and containing 0.020% or less, The balance Fe and workability of good low iron loss non-oriented electrical steel sheet consisting of inevitable impurity elements and a method of manufacturing the same.
机译:[概述] [挑战]是一种应力释放晶粒,尺寸小,退火前的可加工性良好,优异的无取向电工钢板的铁损消失后退火后晶粒的铁显着生长,并提供其制造方法。 A以上,以质量%计,C:0.010%以下,Mn:0.1%。 5%,Si:0.1%或4%以下,Al:0.1%或4%以下,Si + M n + Al≤5.0%,Mg:0.0005%或大于0.020%,甚至Ca:0.0005%或大于或等于Mg + Ca:0.020%或REM:0.005%或以上,Mg + REM:0.020%或以下,或Ca,REM等于或大于0.005%Mg + Ca + REM:含0.020 %Fe以下,由不可避免的杂质元素构成的良好的低铁损无方向性电磁钢板的余量Fe和可加工性及其制造方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号