首页> 外国专利> Adjustment method of copper ion concentration of copper removal electrolytic solution

Adjustment method of copper ion concentration of copper removal electrolytic solution

机译:脱铜电解液中铜离子浓度的调节方法

摘要

PURPOSE:To stabilize the feed flow rate of an electrolyte for removing copper and to carry out appropriate copper removing electrolysis by feeding a part of the anolyte prepared from a waste liquid of nickel electrolysis in nickel refining to the stage where the waste electrolyte is electrolytically decomposed to the copper powder. CONSTITUTION:A nickel matte 1 and elemental sulfur 2 are mixed with a copper-contg. nickel chloride soln. 16c, and the mixture is refined and copper- removed to obtain a copper-contg. nickel slurry 13 and a nickel chloride soln. 11. The soln. 11 is treated in a liq. cleaning stage and a nickel electrolyzing stage 5 to obtain electrolytic nickel 9, and the slurry 13 is treated in a chlorine leaching stage 6 and a copper-removing electrolytic stage 7 to obtain copper powder 10. In the operations, an anolyte 15 is prepared from a waste nickel electrolyte 14, an a part of the anolyte is supplied to a copper-removing electrolyte 18 from the chlorine leaching stage 6 to adjust the copper concn. in the electrolyte 18. As a result, the copper concn. in the electrolyte 18 is lowered without adding water, and the electrolyte is supplied at a stabilized feed flow rate.
机译:目的:通过将镍精炼中镍电解废液制得的部分阳极电解液送入电解废电解液的阶段,以稳定用于去除铜的电解液的进料流量并进行适当的除铜电解。到铜粉。组成:哑光镍1和元素硫2与含铜的混合物混合。氯化镍溶液在图16c中,将混合物精制并除去铜以获得铜接触量。镍浆料13和氯化镍溶液。 11. Soln。 11在液体中处理。清洗阶段和镍电解阶段5来获得电解镍9,并在氯浸出阶段6和脱铜电解阶段7中对浆料13进行处理以获得铜粉10。在操作中,由以下步骤制备阳极电解液15:在废镍电解液14中,将一部分阳极电解液从氯浸出级6供给至除铜电解液18,以调整铜浓度。结果,电解液18中的铜浓度增加。在不添加水的情况下降低电解质18中的电解质,并且以稳定的进料流速供应电解质。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号