PROBLEM TO BE SOLVED: To provide a powder coating film formation method excellent in a finished appearance.;SOLUTION: A characteristic of the powder coating film formation method is to form the coating film, by performing an electrostatic powder coating to a material to be coated so that a density of the powder coating, such as of a vinyl system resin powder coating material, a polyester system powder coating material, an epoxy system resin powder coating, material, becomes 40% or more, and then by heating for the film formation. Moreover, a characteristic of the powder coating film formation method is that a mean particle diameter of the powder of the coating material is 5 to 30 μm, a thermosoftening temperature of the powder coating material is 30 to 100°C, and the powder coating film thickness is 50 to 150 μm.;COPYRIGHT: (C)2003,JPO
机译:解决的问题:提供一种具有优异的外观外观的粉末涂膜形成方法。解决方案:该粉末涂膜形成方法的特征是通过对待涂材料进行静电粉末涂膜来形成涂膜。使乙烯基系树脂粉末涂料,聚酯系粉末涂料,环氧系树脂粉末涂料等粉末涂料的密度为40%以上,然后加热成膜。 。此外,粉末涂膜形成方法的特征在于:涂料的粉末的平均粒径为5至30μm,粉末涂料的热软化温度为30至100℃,并且粉末为粉末。涂膜厚度为50至150μm.COPYRIGHT:(C)2003,JPO

著录项

  • 公开/公告号JP2002320905A

    专利类型

  • 公开/公告日2002-11-05

    原文格式PDF

  • 申请/专利权人 KANSAI PAINT CO LTD;

    申请/专利号JP20010132993

  • 申请日2001-04-27

  • 分类号B05D1/06;C09D5/03;C09D201/00;

  • 国家 JP

  • 入库时间 2022-08-22 00:55:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号