首页> 外国专利> FORMATION DEVICE OF SURFACE MULTIPOLE ANISOTROPIC RING MAGNET AND THE SURFACE MULTIPOLE ANISOTROPIC RING MAGNET

FORMATION DEVICE OF SURFACE MULTIPOLE ANISOTROPIC RING MAGNET AND THE SURFACE MULTIPOLE ANISOTROPIC RING MAGNET

机译:表面多极异性环磁体的形成装置和表面多极异性环磁体的形成装置

摘要

PROBLEM TO BE SOLVED: To prevent cracks from being generated between magnetic poles in a surface multipole anisotropic ring magnet using a ferrite-plate-like particle.;SOLUTION: This formation device is used in a formation process in a magnetic field, when the surface multipole anisotropic ring magnet is manufactured by a sintering method, and has a cylindrical form 3, a sleeve 4, and a core rod 5. In this case, formation space 2 is composed of the inner-periphery surface of the sleeve 4 and the outer-periphery surface of the core rod 5, a region in contact with at least the sleeve 4 in the form 3 is made of a material having high permeability, and the sleeve 4 is made of a non-magnetic material. When the number of poles of the magnet to be manufactured is set to n, n coils 6 for applying a magnetic field exist in the form 3. In the section of the sleeve 4, the inner periphery is set to a circle, at the same time, an outer periphery is set to n-polygon, and each vertex of the n polygon exists between adjacent coils 6 and 6.;COPYRIGHT: (C)2002,JPO
机译:解决的问题:为了防止使用铁氧体板状颗粒的表面多极各向异性环形磁铁的磁极之间产生裂纹;解决方案:该成形装置用于磁场的成形过程中,当表面多极各向异性环形磁铁是通过烧结法制造的,具有圆筒形状3,套筒4和芯棒5。在这种情况下,形成空间2由套筒4的内周面和外部构成。在芯棒5的外周表面上,至少与形式3的套筒4接触的区域由具有高磁导率的材料制成,并且套筒4由非磁性材料制成。当将要制造的磁体的极数设置为n时,以形式3存在用于施加磁场的n个线圈6。在套筒4的截面中,内周部被设置为相同的圆形。此时,将外周设置为n多边形,并且该n多边形的每个顶点都位于相邻的线圈6和6之间; COPYRIGHT:(C)2002,JPO

著录项

  • 公开/公告号JP2002164237A

    专利类型

  • 公开/公告日2002-06-07

    原文格式PDF

  • 申请/专利权人 TDK CORP;

    申请/专利号JP20000358351

  • 申请日2000-11-24

  • 分类号H01F41/02;B22F3/02;H01F1/11;

  • 国家 JP

  • 入库时间 2022-08-22 00:53:50

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号