A heat-resisting steel comprising 0.15-0.30 wt. % C, 0.05-0.3 wt. % Si, 0.01-0.7 wt. % Mn, 1.8-2.5 wt. % Cr, 0.15-0.23 wt. % V, 1.5-2.5 wt. % W, 0.01-0.02 wt. % Ti, 0.01-0.08 wt. % Nb, 0.005-0.03 wt. % N, 0.001-0.015 wt. % B, and Fe and unavoidable impurities as the remainder; a heat-resisting steel comprising 0.15-0.30 wt. % C, 0.05-0.3 wt. % Si, 0.01-0.7 wt. % Mn, 1.8-2.5 wt. % Cr, 0.15-0.23 wt. % V, 1.5-2.5 wt. % W, 0.3-0.8 wt. % Mo, 0.01 -0.02 wt. % Ti, 0.01-0.08 wt. % Nb, 0.005-0.03 wt. % N, 0.001-0.015 wt. % B, and Fe and unavoidable impurities as the remainder; and a heat-resisting steel that is obtained by subjecting one of the above heat-resisting steels to a heat treatment comprising the step of oil-cooling the heat-resisting steel to a temperature of 300° C. or lower. These heat-resisting steels are excellent in both high-temperature strength and impact properties.
机译:包含0.15-0.30重量%的耐热钢。 C,0.05-0.3重量%。 Si,0.01-0.7重量%。 Mn%,1.8-2.5 wt。 Cr%,0.15-0.23 wt。 V,1.5-2.5重量%。 W,0.01-0.02重量%。 Ti的重量百分比为0.01-0.08。 Nb%,0.005-0.03 wt。 N,0.001-0.015重量%。 B,Fe和不可避免的杂质。包括0.15-0.30重量%的耐热钢。 C,0.05-0.3重量%。 Si,0.01-0.7重量%。 Mn%,1.8-2.5 wt。 Cr%,0.15-0.23 wt。 V,1.5-2.5重量%。 W,0.3-0.8重量%。 Mo,0.01-0.02重量%。 Ti的重量百分比为0.01-0.08。 Nb%,0.005-0.03 wt。 N,0.001-0.015重量%。 B,Fe和不可避免的杂质。通过将上述耐热钢之一进行热处理而得到的耐热钢,其包括将耐热钢油冷却至300℃的温度的步骤。 C.或更低。这些耐热钢在高温强度和冲击性能方面均优异。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号