Method for Smelting of Copper sulfide Concentrate, which occurs by oxidation of the Iron Concentrate, with the help of Cao and SiO2 as fluxes.And where the slag produced must meet certain requirements with regard to the weight of Cao, SiO2, and fe feox present in it.

机译:通过Cao和SiO2作为助熔剂通过铁精矿的氧化而发生的硫化铜精矿的冶炼方法,并且所产生的炉渣必须满足有关Cao,SiO2和feox的重量的某些要求在里面。

摘要

Method for Smelting of Copper Sulphide Concentrate essentially includes the steps of: adding the Copper sulfide Concentrate, the basic material of SiO2.Cao and Basic material to melt and bring elconcentrado Sulphide Copper smelting slag by oxidation to produce Product and at least one selected from the group of white metalAnd blister Copper, so that at least part of the Faith in the Copper sulfide Concentrate is transferred to the slagWhile at least part of the SO2 is removed in the form of Copper concentrates and that at least in the form of metal or white blister copper and where the composition of the slag is controlled.So that the weight ratio of CAO / (Si02 + CaO) is in the range between 0.6 and 0.85 while the weight ratio of Fe / (feox + SiO2 + CaO) is in the range of 0.5 to 0.6.
机译:硫化铜精矿的冶炼方法主要包括以下步骤:添加硫化铜精矿,SiO2的基础材料,Cao和碱性材料以熔融并产生Elcentcentrado Sulphide通过氧化生产铜冶炼渣,以生产产品和选自以下的至少一种:一组白色金属和起泡的铜,以便将至少一部分硫化铜精矿中的信仰转移到矿渣中,同时至少以铜精矿的形式除去至少一部分SO2,并且至少以金属或白色的形式除去粗铜和控制炉渣成分的铜,使得CAO /(SiO2 + CaO)的重量比在0.6到0.85之间,而Fe /(Feox + SiO2 + CaO)的重量比为在0.5到0.6的范围内。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号