首页> 外国专利> METHOD FOR CONCENTRATING AND SEPARATING amp;bgr;-2CaO·SiO2 FROM STEELMAKING SLAG

METHOD FOR CONCENTRATING AND SEPARATING amp;bgr;-2CaO·SiO2 FROM STEELMAKING SLAG

机译:从炼钢渣中浓缩分离b 2 CaO·SiO 2的方法

摘要

the present invention is a high value-added steel slag recycling it for -2CaO SiO 2 relates to a method of concentrating and separating . More particularly, the present invention is -2CaO SiO 2 efficiently concentrated and separated from the slag in order to be able to use as a cement admixture -2CaO SiO 2 in slag to a method for enrichment and separation. -2CaO SiO 2 concentration and separation of the method according to an embodiment of the present invention, (a) drying and crushing of slag phase; (B) selecting a first non-complex of the steel-making slag by using a magnetic separator; (C) and the first non-powdered complex, the method comprising: selecting a material of low hardness by using a screen device; And (d) selecting a second non-complex of the material of the low hardness by using a magnetic separator; And (e) using an air classifier is characterized in that it comprises the step of selecting a material of a low specific gravity of the second non-complex. ;
机译:本发明是一种将-2CaO SiO 2 回收利用的高附加值钢渣,它涉及一种浓缩和分离的方法。更特别地,本发明是有效地浓缩和从矿渣中分离出-2CaO SiO 2 ,以便能够在矿渣中将-2CaO SiO 2用作水泥混合物。一种富集和分离的方法。 -2CaO SiO 2 的浓缩和分离的方法,根据本发明的一个实施方案,(a)干燥和粉碎炉渣相; (B)通过使用磁选机选择炼钢渣的第一非复合物; (C)和第一非粉末状复合物,该方法包括:通过使用筛分装置选择低硬度的材料; (d)通过使用磁分离器选择低硬度材料的第二非复合物;并且(e)使用空气分级机的特征在于,其包括选择第二非复合物的低比重的材料的步骤。 ;

著录项

  • 公开/公告号KR101215412B1

    专利类型

  • 公开/公告日2012-12-26

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20100136691

  • 发明设计人 이훈하;조봉석;

    申请日2010-12-28

  • 分类号B02C23/08;C04B5/00;

  • 国家 KR

  • 入库时间 2022-08-21 16:28:00

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号