首页> 外国专利> Water soluble soundproofing. applies a rust prevention coating proposal manufacture method and this material and coating the method which it does

Water soluble soundproofing. applies a rust prevention coating proposal manufacture method and this material and coating the method which it does

机译:水溶性隔音。应用防锈涂层建议的制造方法和该材料并进行涂层的方法

摘要

The present invention relates to a method of coating by applying the manufacturing method and the material of the sound insulation, a water-soluble anti-corrosive coating.; The present invention is a water emulsified state containing 40 to 60% ethylene for this purpose - the vinyl acetate copolymer (ethylene-vinyl acetate copolymer, EVA) into the container to 100% by weight of water herein contain 40 to 60% emulsified state the asphalt from 10 to 50% by weight while put little by little first mixing step of intermixing with a stirring rate of about 500~3000rpm; The second to the first while the of talc (Talc) blowing agent 0.5 to 5% by weight of inorganic additives after the mixing process, and 5-100% by weight of an epoxy resin adhesive, and 5-25% by weight of the ester type, respectively put little by little in order intermix the mixing process; Wherein after the second mixing step plasticizer 0 to 20 it will be made of a third mixing step of mixing a cross-% by weight of surfactant 0-10% by weight.; The present invention constructed as described above is an exemplary so as to obtain an excellent as well as the rust-inhibitive performance sound-absorbing effect to the coating process to various kinds of equipment that require sound insulation and anti-corrosive, will a manner that reduces the air pollution not causing organic volatiles, applied It will shorten the process so that you can get improvements and cost savings, and improve the quality of this product due to the effect of productivity.
机译:本发明涉及一种通过应用隔音材料的制造方法和材料进行涂层的方法,一种水溶性防腐涂层。为此,本发明是一种水乳化态,其含有40至60%的乙烯-乙酸乙烯酯共聚物(乙烯-乙酸乙烯酯共聚物,EVA)进入容器中至100重量%的水在此含有40至60%的乳化态。沥青按重量计从10%至5​​0%,同时逐步进行第一混合步骤,以约500〜3000rpm的搅拌速度进行混合;第二至第一滑石粉(滑石粉)在混合过程后添加0.5-5重量%的无机添加剂,5-100重量%的环氧树脂胶粘剂和5-25重量%的滑石粉。酯型,分别一点一点地依次混合以混合过程;其中,在第二混合步骤增塑剂0至20之后,将由第三混合步骤制成,所述第三混合步骤将0-10重量%的交叉表面活性剂混合。如上所述构造的本发明是示例性的,以便获得对需要隔音和防腐蚀的各种设备的涂覆过程的优异的以及防锈性能的吸音效果。减少不会造成有机挥发物的空气污染,适用它将缩短过程,以便您可以得到改进并节省成本,并且由于生产率的影响而提高了该产品的质量。

著录项

  • 公开/公告号KR20010103099A

    专利类型

  • 公开/公告日2001-11-23

    原文格式PDF

  • 申请/专利权人 신원범;

    申请/专利号KR20010059400

  • 申请日2001-09-25

  • 分类号C09D5/08;

  • 国家 KR

  • 入库时间 2022-08-22 00:32:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号