The present invention relates to a method of coating by applying the manufacturing method and the material of the sound insulation, a water-soluble anti-corrosive coating.; The invention water is emulsified state of ethylene containing 40 to 60% for this purpose - in an emulsified state into a vinyl acetate copolymer (ethylene-vinyl acetate copolymer, EVA) 100 parts by weight of the water vessel here contains 40 to 60% 10 to 50 parts by weight of asphalt while little by little into the first mixing step of intermixing with a stirring rate of about 500~3000rpm; Wherein the first mixing step after the foaming agent giving from 0.5 to 5 parts by weight of inorganic additive talc (Talc) 5~100 parts by weight, respectively, and put little by little, as the adhesive resin 5 to 25 parts by weight of the order of the epoxy and ester type second mixture to intermix fair; The first will be made of a third mixing step of mixing two mutually mixing process after 0 to 20 parts by weight of a plasticizer and 0 to 10 parts by weight of surface active agent.; The present invention constructed as described above is an exemplary so as to obtain an excellent as well as the rust-inhibitive performance sound-absorbing effect to the coating process to various kinds of equipment that require sound insulation and anti-corrosive, will a manner that reduces the air pollution not causing organic volatiles, applied It will shorten the process so that you can get improvements and cost savings, and improve the quality of this product due to the effect of productivity.
机译:本发明涉及一种通过应用隔音材料的制造方法和材料进行涂层的方法,一种水溶性防腐涂层。为此,本发明的水是包含40至60%的乙烯的乳化态-在乳化态下成为乙酸乙烯酯共聚物(乙烯-乙酸乙烯酯共聚物,EVA),按重量计,水容器100重量份中包含40至60%10至50重量份的沥青,同时逐渐以约500〜3000rpm的搅拌速度进入第一混合步骤;其中在起泡剂后的第一混合步骤中分别加入0.5-5重量份的无机添加剂滑石粉(滑石粉)5〜100重量份,并作为粘合剂树脂5-25重量份环氧和酯型第二种混合物的相互混合顺序;第一将由第三混合步骤制成,该第三混合步骤在0至20重量份的增塑剂和0至10重量份的表面活性剂之后将两个相互混合的过程混合。如上所述构造的本发明是示例性的,以便获得对需要隔音和防腐蚀的各种设备的涂覆过程的优异的以及防锈性能的吸音效果。减少不会造成有机挥发物的空气污染,适用它将缩短过程,以便您可以得到改进并节省成本,并且由于生产率的影响而提高了该产品的质量。

著录项

  • 公开/公告号KR100480511B1

    专利类型

  • 公开/公告日2005-03-31

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20010059400

  • 申请日2001-09-25

  • 分类号C09D5/08;

  • 国家 KR

  • 入库时间 2022-08-21 22:04:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号