首页> 外国专利> A process for the preparation of a hydraulically bound thin flat protective layer for the repair of damaged concrete structures, in particular of steel concrete constructions

A process for the preparation of a hydraulically bound thin flat protective layer for the repair of damaged concrete structures, in particular of steel concrete constructions

机译:制备水硬性薄保护层的方法,用于修复受损的混凝土结构,特别是钢混凝土结构

摘要

The invention relates to a method for production and processing of a cement-bonded protective layer for the repair of damaged concrete structures, in particular of steel concrete constructions. Dollars a of the invention the object of the invention is a disadvantage of the prior art owing to eliminate the content of the patent claims. In particular state of the present invention to provide a hydraulic thin surfaces renovation mixture with a high tightly - and adhesion to develop. Dollars a this is achieved according to the invention in that the cement-bound protective layer as a carbon dioxide - and / or moisture barrier with the use of a grind - mixture in a layer thickness of 3 - 8 mm to the damaged or carbonated concrete surfaces is applied, wherein the particle fraction of the binder, 1 mu m, is strongly increased and the particle fraction of the binder to 10 mu m compared with conventional cement is reduced, so that by means of a targeted reduction of the capillary - and, on the one hand, a diffusion gelporengefüges reduced, and on the other hand an additional subsequent real calibrating process is achieved to the right.
机译:用于水泥粘结的保护层的生产和加工方法技术领域本发明涉及一种用于水泥粘结的保护层的生产和加工的方法,用于修复受损的混凝土结构,特别是钢混凝土结构。发明内容由于消除了专利权利要求的内容,本发明的目的是现有技术的缺点。在本发明的特定状态下,提供了具有高紧密性和粘附力的水硬性薄表面翻新混合物。根据本发明,这是通过水泥结合的保护层作为二氧化碳和/或湿气屏障而实现的,该保护层使用碾磨的混合物,其厚度为受损的或碳酸化的混凝土的3-8mm施加表面,其中与传统的水泥相比,粘合剂的颗粒分数(1微米)大大增加,粘合剂的颗粒分数降至10微米,从而通过有针对性地减少毛细管-和一方面减少了扩散凝胶的形成,另一方面又在右侧实现了其他后续的实际校准过程。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号