首页> 外国专利> COMBINING METHOD AND ITS COMBINING MATERIAL OF POSITIVE ELECTRODE ACTIVE MATERIAL FOR NONAQUEOUS LITHIUM SECONDARY BATTERY AND CONDUCTIVE SUBSIDIARY MATERIAL, AND POSITIVE ELECTRODE AND NONAQUEOUS LITHIUM SECONDARY BATTERY USING THE SAME

COMBINING METHOD AND ITS COMBINING MATERIAL OF POSITIVE ELECTRODE ACTIVE MATERIAL FOR NONAQUEOUS LITHIUM SECONDARY BATTERY AND CONDUCTIVE SUBSIDIARY MATERIAL, AND POSITIVE ELECTRODE AND NONAQUEOUS LITHIUM SECONDARY BATTERY USING THE SAME

机译:非均质锂二次电池和导电性次要材料的正电极活性材料及正电极和非均质锂二次电池的结合方法及其组合材料

摘要

PPROBLEM TO BE SOLVED: To improve dispersibility of a positive electrode material and a conductive subsidiary material (carbon powder) and make an initial capacity of a positive electrode of a nonaqueous lithium secondary battery and discharging rate characteristics better than a conventional one. PSOLUTION: A positive electrode active material, a conductive subsidiary material (carbon powder), a solvent and a binder are mixed to make up a slurry, which is spray dried to obtain a complex material of the positive electrode active material and the conductive subsidiary material. The spray drying is made at 100 to 350C by a spray dryer, which makes up a complex material with the positive electrode active material held around the carbon powder. Then, after a solvent with a binder dissolved in it is added to and kneaded with the complex material, it is coated on and pressed to a metal foil and dried to make up a positive electrode. PCOPYRIGHT: (C)2003,JPO
机译:

要解决的问题:与以往相比,提高正极材料和导电辅助材料(碳粉)的分散性,并使非水锂二次电池的正极的初始容量和放电速率特性更好。

解决方案:将正极活性材料,导电辅助材料(碳粉),溶剂和粘合剂混合以制成浆液,然后将其喷雾干燥,以得到正极活性材料与负极活性物质的复合材料。导电辅助材料。喷雾干燥通过喷雾干燥器在100至350℃下进行,该喷雾干燥器构成复合材料,并且正极活性物质保持在碳粉周围。然后,在将溶解有粘合剂的溶剂加入到复合材料中并与之混合后,将其涂布并压在金属箔上并干燥以构成正极。