首页> 外国专利> CATHODE CONTAINER FOR SODIUM - SULFUR BATTERY, METHOD FOR FORMING SPRAYED COATING ON INNER CIRCUMFERENTIAL SURFACE OF CATHODE CONTAINER, AND QUALITY JUDGMENT METHOD FOR SPRAYED COATING

CATHODE CONTAINER FOR SODIUM - SULFUR BATTERY, METHOD FOR FORMING SPRAYED COATING ON INNER CIRCUMFERENTIAL SURFACE OF CATHODE CONTAINER, AND QUALITY JUDGMENT METHOD FOR SPRAYED COATING

机译:钠硫电池的阴极容器,在阴极容器内圆周表面上形成喷涂层的方法以及喷涂层的质量判断方法

摘要

PPROBLEM TO BE SOLVED: To provide a cathode container for a sodium - sulfur battery having sprayed coating for corrosion protection having high corrosion resistance and high durability. PSOLUTION: In the cathode container for the sodium - sulfur battery having the sprayed coating on the inner circumferential surface, cross section metallographic structure of 10 m unit of thickness of the sprayed coating is dense lamellar structure 3 comprising at least three flat sprayed particles 1. The sprayed coating on the inner circumferential surface of the cathode container for the sodium - sulfur battery is Cr-Fe alloy powder containing 65% or more Cr, containing 1.5% or less OSB2/SBin metal powder, and is formed by plasma spraying in the atmosphere metal powder for spray coating which is crushed massive metal powder having a particle size of 75 m or less. PCOPYRIGHT: (C)2003,JPO
机译:

要解决的问题:提供用于钠-硫电池的阴极容器,该阴极容器具有用于腐蚀防护的喷涂涂层,具有高耐腐蚀性和高耐久性。

解决方案:在用于钠-硫电池的阴极容器的内周表面上具有喷涂层的阴极容器中,喷涂层厚度为10 m单位的横截面金相组织为致密的层状结构3,该层状结构3包括至少三个扁平喷涂层颗粒1.在钠硫电池阴极容器内周表面上喷涂的涂层是Cr-Fe合金粉末,其金属含量在65%以上,O 2 在1.5%以下粉末,是通过在大气中进行等离子喷涂而形成的,用于喷涂的金属粉末是压碎的,粒径为75 m以下的块状金属粉末。

版权:(C)2003,日本特许厅

著录项

  • 公开/公告号JP2003243025A

    专利类型

  • 公开/公告日2003-08-29

    原文格式PDF

  • 申请/专利权人 NGK INSULATORS LTD;

    申请/专利号JP20020040183

  • 发明设计人 ANDO TAKASHI;

    申请日2002-02-18

  • 分类号H01M10/39;C23C4/08;H01M2/02;

  • 国家 JP

  • 入库时间 2022-08-22 00:17:21

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号