首页>
外国专利>
METHOD FOR FORECASTING PLATE CROWN IN HOT ROLLING AND HOT ROLLING METHOD
METHOD FOR FORECASTING PLATE CROWN IN HOT ROLLING AND HOT ROLLING METHOD
展开▼
机译:热轧中板面变形的预测方法及热轧方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
PROBLEM TO BE SOLVED: To forecast a plate crown with a high degree of accuracy and at a small calculation load even under rolling conditions wherein a non-contact area arises between a work roll and a backup roll. ;SOLUTION: Under a plurality of rolling conditions, the plate crown is calculated (S110), considering (S106, S109) contact area information using a splitting model and the plate crown (S110) is obtained by the plate crown forecasting formulas (A), (B) decided based on the calculation resu Crout/Hout=ζηCM/Hout+ηCrin/Hin...(A) CM=αP.P+αB.FB+αCW.CRW+αCB.CRB+αCH.CRH...(B) Here, mechanical crown is indicated as CM, rolling load as P, bending force as FB, work roll initial crown as CRW, backup roll crown CRB, work roll thermal crown as CRH, and influence coefficient as αP, αB, αCW, αCB, αCH.;COPYRIGHT: (C)2003,JPO
展开▼
机译:解决的问题:即使在轧制条件下工作辊和支撑辊之间都出现非接触区域的情况下,以高精度和小计算量预测板凸度。 ;解决方案:在多个轧制条件下,使用分裂模型考虑(S106,S109)接触面积信息,计算板凸度(S110),并通过板凸度预测公式(A)获得板凸度(S110) ,(B)根据计算结果确定; Cr out Sub> / H out Sub> =ζη CM / H out Sub> +&etaCrin / H in Sub>。 ..(A)CM =αP.P+αB.FB+αCW.CRW+αCB.CRB+αCH.CRH...(B)在此,机械胎冠表示为CM ,轧制载荷为P,弯曲力为FB,工作辊初始凸度为CRW,支承辊凸度CRB,工作辊热凸度为CRH,影响系数为αP,αB,αCW,αCB, α CH.COPYRIGHT:(C)2003,JPO
展开▼