PROBLEM TO BE SOLVED: To provide superfluid mortar of excellent fluidity immediately after kneading, and excellent workability dissolving the delay of a construction period by preparing and kneading a superfluid admixture in a plant mixed and kneaded mortar or a site mixed and hand-kneaded mortar transported by a mixer truck, which was heretofore impossible, further at a construction site.;SOLUTION: In this method of manufacturing the supefluid mortar, the superfluid admixture comprising a fluidizing agent, an AE water reducing agent, a highly efficient AE water reducing agent, and a commonly used thickener, expanding agent, defoaming agent and reaction control agent, is mixed and stirred in a mortar base material of the plant mixed and kneaded mortar or site mixed and hand-kneaded mortar formed of an admixture of water, coarse sand, silica sand, cement, fly ash, and the like, further at the construction site.;COPYRIGHT: (C)2003,JPO
机译:解决的问题:在混炼后的砂浆或现场混运的手工混炼的砂浆中制备和混炼超流质掺合料,以便在捏合后立即提供流动性极佳的超流质砂浆,并具有优异的可加工性,从而解决了施工周期的延迟。解决方案:在这种制造超流体砂浆的方法中,超流体混合物包括流化剂,AE减水剂,高效AE减水剂,然后,将常用的增稠剂,膨胀剂,消泡剂和反应控制剂在由植物和研钵混合而成的研钵基料中或在由水,粗砂,硅砂,水泥,粉煤灰等在施工现场的更远处。;版权所有:(C)2003,日本特许厅

著录项

  • 公开/公告号JP2003120008A

    专利类型

  • 公开/公告日2003-04-23

    原文格式PDF

  • 申请/专利权人 TAKASHIMA YASUO;

    申请/专利号JP20010318258

  • 发明设计人 TAKASHIMA YASUO;

    申请日2001-10-16

  • 分类号E04F15/12;

  • 国家 JP

  • 入库时间 2022-08-22 00:15:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号