首页> 外国专利> METHOD FOR PREPARING IN AN AQUEOUS EMULSION A BITUMEN/POLYMER BINDER WITH CONTINUOUS TRIDIMENSIONAL POLYMER STRUCTURE AND APPLICATION OF SUCH BINDER FOR COATINGS OR COVERINGS

METHOD FOR PREPARING IN AN AQUEOUS EMULSION A BITUMEN/POLYMER BINDER WITH CONTINUOUS TRIDIMENSIONAL POLYMER STRUCTURE AND APPLICATION OF SUCH BINDER FOR COATINGS OR COVERINGS

机译:具有连续三维聚合物结构的乳液/水乳液/聚合物粘合剂的制备方法及该粘合剂在涂料或覆盖层中的应用

摘要

it leads to the formation of a zone of asphalt emulsion (i) a polymer componentthe sulfur which is cross linkable.in the form of a molten mass having a temperature of 100 degrees celsius.230 degrees, and a viscosity of at most z (to the stp.(ii) an aqueous phase containing a) an emulsifier and witha temperature of 10 degrees and 90 degrees c, and (iii) a sys -the crosslinking system at an appropriate level of sulphur donor reportsweight of the bitumen / polymer component in phasewater from 30: 10 to 85: 15, and the reaction mixture is maintained andin the area of training, training of the emulsion.a temperature between 50 degrees and 100 degrees c, to obtain abitumen emulsion binder polymer in which the polymer of thebinder is cross-linked in a three-dimensional structure. the emulsion obtained iscan be used for the realization of the road surfaces.coating of coated or waterproof.
机译:它导致形成沥青乳液区域(i)聚合物组分可交联的硫。以温度为100摄氏度的熔融物质的形式存在。230度,最高粘度z(至stp。(ii)水相,其包含a)乳化剂和温度为10摄氏度和90摄氏度,以及(iii)sys-适当水平的硫供体报告下的交联体系相中沥青/聚合物成分的重量将水的比例从30:10到85:15,并保持反应混合物在培训领域,乳液的培训。温度在50到100摄氏度之间,以获得沥青乳液粘合剂聚合物,其中的聚合物粘合剂以三维结构交联。得到的乳液是可用于实现路面。涂层的涂层或防水。

著录项

  • 公开/公告号CA2065727C

    专利类型

  • 公开/公告日2003-05-13

    原文格式PDF

  • 申请/专利权人 ELF FRANCE;

    申请/专利号CA19912065727

  • 发明设计人 CHAVEROT PIERRE;DEMANGEON FRANCIS;

    申请日1991-07-18

  • 分类号C08L95/00;

  • 国家 CA

  • 入库时间 2022-08-21 23:58:55

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号