Fire-resistant welding steel in the form of hollow profiles, supports or molded steel contains (in wt.%) 0.06-0.13 C, 0.15-0.50 Si, 1.0-2.0 Mn, maximum 0.025 P, maximum 0.02 S, 0.005-0.040 Al, 0.20-0.40 Mo, 0.40-0.70 W, 0.02-0.05 Nb and a balance of Fe with unavoidable impurities. A component made from the steel has a yield point at elevated temperature of at least 200 MPa at 600 degrees C and a CEIIW value of less than 0.5. ??An Independent claim is also included for a process for the production of hot-rolled hollow profiles having a thickness of up to 30 mm made from the above steel comprising casting the steel into strands, hot rolling into rods and then into hollow profiles at at least 1200 degrees C before cooling in air.
机译:中空型材,支撑件或模制钢形式的耐火焊接钢包含(重量%)0.06-0.13 C,0.15-0.50 Si,1.0-2.0 Mn,最大0.025 P,最大0.02 S,0.005-0.040 Al ,0.20-0.40 Mo,0.40-0.70 W,0.02-0.05 Nb以及余量的Fe和不可避免的杂质。由钢制成的部件在600摄氏度下的高温屈服点至少为200 MPa,CEIIW值小于0.5。由上述钢制成的厚度不超过30mm的热轧空心型材的生产方法也包括独立权利要求,包括将钢铸成钢绞线,热轧成棒材然后成空心在空气中冷却之前,至少要在1200摄氏度以下进行轮廓分析。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号