PURPOSE: A method for preparing a delaminating acrylate resin/layered silicate nanocomposite and a delaminating acrylate resin/layered silicate nanocomposite prepared by the method are provided, to enable a delaminating acrylate resin/layered silicate nanocomposite to be prepared by emulsion polymerization without substituting the polar surface of layered silicate having bad affinity to a polymer with a nonpolar organic compound. CONSTITUTION: The method comprises the steps of adding an acrylate resin monomer, an initiator and a reactive emulsifying agent to a layered silicate dispersion solution, and polymerizing the mixture to prepare a polymer; and adding a monomer to the polymer and post-polymerizing the mixture. Preferably the layered silicate is at least one selected from the group consisting of montmorillonite, hectorite, fluorohectorite and saponite; and the acrylate resin monomer is at least one selected from the group consisting of methyl methacrylate, methacrylate, methyl acrylate, butyl methacrylate, butyl acrylate and isooctyl acrylate. The content of the layered silicate in the nanocomposite is 0.1-10 wt%.
机译:目的:提供一种制备脱层丙烯酸酯树脂/层状硅酸盐纳米复合材料的方法和通过该方法制备的脱层丙烯酸酯树脂/层状硅酸盐纳米复合材料,以使得能够通过乳液聚合制备脱层丙烯酸酯树脂/层状硅酸盐纳米复合材料而无需取代极性。对具有非极性有机化合物的聚合物具有不良亲和力的层状硅酸盐表面。组成:该方法包括以下步骤:将丙烯酸酯树脂单体,引发剂和反应性乳化剂添加到层状硅酸盐分散液中,并使混合物聚合以制备聚合物。向该聚合物中加入单体并对该混合物进行后聚合。优选地,层状硅酸盐是选自蒙脱石,锂蒙脱石,氟锂蒙脱石和皂石中的至少一种。丙烯酸酯树脂单体是选自甲基丙烯酸甲酯,甲基丙烯酸酯,丙烯酸甲酯,甲基丙烯酸丁酯,丙烯酸丁酯和丙烯酸异辛酯中的至少一种。纳米复合材料中层状硅酸盐的含量为0.1-10重量%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号