PURPOSE: A method for recycling the residual slip casting castable using dolomite and slag is provided which not only contributes to reduction of waste by recycling the residual slip casting castable, but also reduces construction cost and period by increasing interfacial adhesion between residual and new slip casting castables. CONSTITUTION: The recycling method of residual slip casting castable using dolomite and slag comprises the steps of forming a slag coating layer having thickness of 3 to 10 mm on the surface of the residual slip casting castable of the inner wall of the ladle by tilting the ladle after mixing the dolomite raw material with the ladle slag by injecting the dolomite raw material into ladle so that ladle slag generated after skimming slag of molten steel and dolomite raw material are mixed in a weight ratio of 70:1 to 90:1; cooling the ladle to an ordinary temperature, and constructing new slip casting castable to a thickness of 50 to 70 mm on the slag coating layer; and preheating the ladle to a temperature of 1,000 to 1,200 deg.C.
机译:目的:提供一种回收利用白云石和矿渣的残余滑模铸件的方法,该方法不仅有助于通过循环利用残余滑模铸件来减少浪费,而且还可以通过增加残余与新滑模铸件之间的界面粘合力来降低施工成本和周期。浇铸物。构成:利用白云石和矿渣浇铸的渣浆浇铸料的循环利用方法包括以下步骤:通过倾斜钢包,在钢包内壁的渣浆浇铸料的表面上形成厚度为3mm至10mm的炉渣涂层。将白云石原料注入钢包,将白云石原料与钢包渣混合后,将钢水和白云石原料撇渣后产生的钢包渣以70:1〜90:1的重量比混合。将钢包冷却至常温,并在炉渣涂层上构建可浇铸成厚度为50至70毫米的新粉浆铸件。将钢包预热至1,000至1,200℃。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号