首页> 外国专利> Removing impurity alloying components from an aluminum cast alloy comprises completely melting the cast alloy, mixing with boron, casting the melt, and removing or retaining solids produced from the melt before or during casting

Removing impurity alloying components from an aluminum cast alloy comprises completely melting the cast alloy, mixing with boron, casting the melt, and removing or retaining solids produced from the melt before or during casting

机译:从铝铸造合金中去除杂质合金成分包括完全熔化铸造合金,与硼混合,铸造熔体以及在铸造之前或铸造过程中除去或保留由熔体产生的固体。

摘要

Removing impurity alloying components from an aluminum cast alloy comprises completely melting the cast alloy; mixing with 0.005 weight % boron for the purpose of cleaning; casting the melt for a time sufficient for the boron to react with the impurity alloying components; and removing or retaining solids produced from the melt before or during casting. Preferred Features: Boron is added in the form of an aluminum-boron pre-alloy. Reaction time is at least one hour. The aluminum cast alloy is further treated for the purpose of grain refinement.
机译:从铝铸造合金中去除杂质合金成分包括完全熔化铸造合金;以及从铸造合金中去除杂质合金成分。与0.005重量%的硼混合以进行清洁;浇铸熔体的时间足以使硼与杂质合金成分反应;在铸造之前或铸造过程中,除去或保留由熔体产生的固体。首选功能:硼是以铝硼预合金的形式添加的。反应时间至少为一小时。为了细化晶粒,进一步处理了铝铸造合金。

著录项

  • 公开/公告号DE10157722A1

    专利类型

  • 公开/公告日2003-06-05

    原文格式PDF

  • 申请/专利权人 BAYERISCHE MOTOREN WERKE AG;

    申请/专利号DE2001157722

  • 发明设计人 LOHREY UTE;

    申请日2001-11-24

  • 分类号C22C21/00;C22C1/03;C22C1/02;

  • 国家 DE

  • 入库时间 2022-08-21 23:42:26

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号