This invention provides a method for stably adding a predetermined amount of supercritical carbon dioxide at a fixed delivery rate into a forming machine and also a process for producing an expanded thermoplastic resin product by making use of the addition method. Carbon dioxide is charged from a liquefied carbon dioxide cylinder (1) into a predetermined amount deliverable pump (2) while allowing the carbon dioxide to remain in a liquefied state. When the carbon dioxide is pressurized and delivered by the predetermined amount deliverable pump (2), a delivery pressure of the carbon dioxide is controlled at an optional pressure within a range of from a critical pressure (7.4 MPa) of carbon dioxide to 40 MPa to deliver the carbon dioxide without any fluctuation of the amount of the delivery by setting up the pressure of a pressure control valve (3). The carbon dioxide is heated to a critical temperature (31° C.) of carbon dioxide or higher to convert it into supercritical carbon dioxide. This supercritical carbon dioxide is then added to a molten thermoplastic resin in the forming machine (4).
机译:本发明提供了一种以固定的输送速率将预定量的超临界二氧化碳稳定地添加到成形机中的方法,以及通过使用该添加方法来生产膨胀的热塑性树脂产品的方法。将二氧化碳从液化二氧化碳气瓶( 1 )装入预定量的可输送泵( 2 )中,同时使二氧化碳保持液化状态。当通过预定量的可输送泵( 2 )加压并输送二氧化碳时,将二氧化碳的输送压力控制在临界压力(7.4 MPa)范围内的任意压力下。通过设置压力控制阀( 3 )的压力,将二氧化碳输送至40 MPa,以输送二氧化碳而输送量没有任何波动。将二氧化碳加热到二氧化碳的临界温度(31℃)或更高,以将其转化成超临界二氧化碳。然后将这种超临界二氧化碳添加到成型机( 4 )中的熔融热塑性树脂中。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号