PROBLEM TO BE SOLVED: To enhance the production efficiency of lightweight concrete using aggregate low in water content.;SOLUTION: When lightweight concrete is manufactured through a dry mixing process S40 and a kneading process S50 by using artificial lightweight aggregate with a water content of 5% or below, correction water and kneading/mixing water are collectively charged in the kneading process S50 to reduce supply labor of water. In the dry mixing process S40, correction water is not charged at all. Further, the amount of correction water is prescribed as an amount estimated to be absorbed within the manufacturing time from the start of the kneading process S50 to the completion of the finishing process S70.;COPYRIGHT: (C)2004,JPO&NCIPI
机译:解决的问题:使用含水量低的骨料提高轻质混凝土的生产效率;解决方案:通过干混合工艺S40和捏合工艺S50通过使用含水量为5的人造轻质骨料生产轻质混凝土时在捏合步骤S50中,将校正水和捏合/混合水集中加入或低于%(%)以减少水的供应劳动。在干混合过程S40中,完全不添加校正水。此外,将校正水的量规定为在从捏合过程S50开始到完成过程S70完成的制造时间内估计要吸收的量。版权所有:(C)2004,JPO&NCIPI

著录项

  • 公开/公告号JP2004268362A

    专利类型

  • 公开/公告日2004-09-30

    原文格式PDF

  • 申请/专利权人 FUJITA CORP;

    申请/专利号JP20030060784

  • 发明设计人 SHIODA HIROYUKI;

    申请日2003-03-07

  • 分类号B28C7/04;E04C2/04;

  • 国家 JP

  • 入库时间 2022-08-21 23:33:48

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号