首页> 外国专利> It is superior in resistance part corrosiveness and production manner null of the aluminum alloy extruding item whose fatigue strength

It is superior in resistance part corrosiveness and production manner null of the aluminum alloy extruding item whose fatigue strength

机译:疲劳强度高的铝合金挤压件的阻力部分腐蚀性和生产方式优异

摘要

PROBLEM TO BE SOLVED: To provide an aluminum alloy plastic product capable of suppressing the progress of partial corrosion linearly extending to the deep part on the inside of the material and excellent in partial corrosion resistance and fatigue strength.;SOLUTION: This product contains, by weight, 0.2 to 1.2% Si, 0.35 to 1.5% Mg and ≤0.20% Ti and/or 0.3% V, and the balance substantial Al. In the cross- section parallel to the plastic working direction, Ti and/or V high concentration parts and Ti and/or V low concentration parts extending to the plastic working direction in the cross-section parallel to the plastic working direction are superimposed in layers. The Ti and/or V high concentration parts are preferably the ones having an area ratio of 45 to 95% in the cross-section parallel to the plastic working direction. It is produced by casting the molten metal of an alloy at a molten metal cooling rate of ≥5°C/sec, subjecting the obtd. ingot to homogenizing treatment at 520 to 580°C for 1 to 8 hr, executing plastic working after cooling, transforming the cast crystal grains into layers and moreover executing heat treatment for improving its mechanical strength.;COPYRIGHT: (C)2000,JPO
机译:要解决的问题:提供一种铝合金塑料产品,该产品能够抑制部分腐蚀线性延伸到材料内部深处的过程,并且具有优异的部分耐腐蚀性和疲劳强度。重量:0.2至1.2%的Si,0.35至1.5%的Mg和0.20%的Ti和/或0.3%的V,其余部分为Al。在平行于塑性加工方向的截面中,在平行于塑性加工方向的截面中向塑性加工方向延伸的Ti和/或V高浓度部分和Ti和/或V低浓度部分被层叠。 。 Ti和/或V高浓度部分优选是在平行于塑性加工方向的横截面中具有45至95%的面积比的部分。它是通过以〜5℃/秒的熔融金属冷却速率铸造合金熔融金属而制得的。铸锭要在520至580°C下进行均质处理1至8 hr,冷却后进行塑性加工,将铸造的晶粒转变为层状,然后进行热处理以提高其机械强度。;版权:(C)2000,JPO

著录项

  • 公开/公告号JP3552608B2

    专利类型

  • 公开/公告日2004-08-11

    原文格式PDF

  • 申请/专利权人 日本軽金属株式会社;

    申请/专利号JP19990266619

  • 发明设计人 谷津倉 政仁;岡庭 茂;

    申请日1999-09-21

  • 分类号C22F1/05;C22C21/02;C22C21/06;

  • 国家 JP

  • 入库时间 2022-08-21 23:27:28