首页> 外国专利> HIGHLY WEATHER RESISTANT MAGNET POWDER, RESIN COMPOSITION FOR BONDED MAGNET AND BONDED MAGNET OBTAINED BY USING THE RESIN COMPOSITION

HIGHLY WEATHER RESISTANT MAGNET POWDER, RESIN COMPOSITION FOR BONDED MAGNET AND BONDED MAGNET OBTAINED BY USING THE RESIN COMPOSITION

机译:高耐候性磁铁粉末,粘结磁铁的树脂组成和使用该树脂组成的粘结磁铁

摘要

PROBLEM TO BE SOLVED: To provide a highly weather resistant magnet powder having stable and high coercive force and high weather resistance and reduced at its dispersion of coercive force and weather resistance, a resin composition for a bonded magnet and the bonded magnet using the resin composition.;SOLUTION: In the highly weather resistant magnet powder constituted of coating the surface of rare earth element-iron-nitrogen (R-T-N) magnet powder having Th2Zn17 or Th2Ni17 crystal structure with a phosphate (R-T-P-O) film, average grain size is 1-10μm and the composition consists of 20-25 wt% R (rare earth elements), 2.1-3.9 wt% N (nitrogen), 0.2-2.0 wt% P (phosphorus), 0.5-5.0 wt% O (oxygen), and balance T (transition metallic elements and unavoidable impurities) and the content of H (hydrogen) which is an unavoidable impurity is ≤ 0.3wt%.;COPYRIGHT: (C)2004,JPO
机译:解决的问题:为了提供具有稳定且高的矫顽力和高耐候性并且在其矫顽力和耐候性的分散性方面降低的高耐候性磁体粉末,用于粘结磁体的树脂组合物和使用该树脂组合物的粘结磁体解决方案:在高耐候性磁铁粉末中,该磁铁粉末的表面涂覆有Th 2 Zn 17 或Th的稀土元素-铁-氮(RTN)磁铁粉末具有磷酸盐(RTPO)膜的 2 Ni 17 晶体结构,平均晶粒尺寸为1-10μm,组成为20-25 wt%R(稀土)元素),2.1-3.9重量%的N(氮),0.2-2.0重量%的P(磷),0.5-5.0重量%的O(氧)和余量T(过渡金属元素和不可避免的杂质)和H的含量氢)是不可避免的杂质。 0.3wt%.;版权:(C)2004,日本特许厅

著录项

  • 公开/公告号JP2004111515A

    专利类型

  • 公开/公告日2004-04-08

    原文格式PDF

  • 申请/专利权人 SUMITOMO METAL MINING CO LTD;

    申请/专利号JP20020269801

  • 申请日2002-09-17

  • 分类号H01F1/06;B22F1/00;B22F1/02;B22F3/00;B22F3/02;C22C38/00;C22C38/10;H01F1/053;H01F1/08;H01F41/02;

  • 国家 JP

  • 入库时间 2022-08-21 23:27:11