PROBLEM TO BE SOLVED: To provide a method for producing a half-melted billet of an Al alloy for transporting machines, in which the process is simple, the cost reduction of cost is achieved, and the uniform products is obtained.;SOLUTION: An Al alloy having a composition containing, by weight, ≤0.5% Cu, 5.0 to 10% Si, 0.2 to 0.7% Mg, ≤0.35% Zn, ≤0.55% Fe, ≤0.5% Mn and 0.005 to 0.5% Ti, and the balance substantially Al is produced, next, work strain is introduced by cold form forging at a strain ratio of 10 to 40% at a work introducing rate of ≤10 mm/sec. at ≤200°C, and after that, the alloy is held at 576 to 585°C.;COPYRIGHT: (C)2001,JPO
展开▼
机译:解决的问题:提供一种用于运输机器的铝合金的半熔铸坯的生产方法,该方法简单,成本降低,并且获得了均匀的产品。具有按重量计包含小于0.5%的Cu,5.0至10%的Si,0.2至0.7%的Mg,小于0.35%的Zn,小于0.55%的Fe,小于0.5%的Mn和0.005至0.5%的组成的铝合金Ti,并产生基本平衡的Al,然后,通过冷成形锻造以10至40%的应变率以10 mm / sec的应变率引入工作应变。于200°C加热,此后将合金保持在576至585°C.COPYRIGHT:(C)2001,JPO
展开▼