首页> 外国专利> METHOD OF PROTECTION AGAINST CORROSION OF A STEEL DETAIL, MANUFACTURED FROM AUSTENITIC OR SEMI-SUSTAINED STEEL, DURING SULFURIC ACID ACQUISITION

METHOD OF PROTECTION AGAINST CORROSION OF A STEEL DETAIL, MANUFACTURED FROM AUSTENITIC OR SEMI-SUSTAINED STEEL, DURING SULFURIC ACID ACQUISITION

机译:硫酸采集过程中用奥氏体或半持续钢铁制造的钢材腐蚀的防护方法。

摘要

This invention relates to a method for the protection against corrosion of steel parts made of austenitic or semi-austenitic steel during the production of sulfuric acid. To improve the corrosion resistance of steel parts that are in contact with sulfuric acid, it is proposed to use austenitic or semi-austenitic steel, the Cr content of which is in the range from 15 to 31 wt.%, And the Ni content is in the range from 9 to 60 wt.% and where the ratio of the quantities of chemical elements (Cr + Si) / (Ni + Mo) is in the range from 0.9 to 1.9 or where the ratio of the quantities of chemical elements Cr / (Ni + Mo) is in the range from 0.8 to 1 , 5, and additionally provide this steel part with protection against anodic corrosion. People application was published together with the international search report.
机译:本发明涉及一种在硫酸生产过程中防止由奥氏体或半奥氏体钢制成的钢零件腐蚀的方法。为了提高与硫酸接触的钢部件的耐腐蚀性,建议使用奥氏体或半奥氏体钢,其Cr含量在15至31wt。%的范围内,并且Ni含量为在9-60wt。%的范围内,并且其中化学元素的量(Cr + Si)/(Ni + Mo)的比例在0.9-1.9的范围内,或者其中化学元素Cr的量的比例/(Ni + Mo)的范围为0.8到1、5,并且还为该钢部件提供了抗阳极腐蚀的保护。人员申请与国际搜索报告一起发布。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号