首页> 外国专利> microporous crystalline zeolite material (ITQ-20) and its method of obtention.

microporous crystalline zeolite material (ITQ-20) and its method of obtention.

机译:微孔晶体沸石材料(ITQ-20)及其观察方法。

摘要

microporous crystalline zeolite material (ITQ-20) and its preparation process.; A microporous crystalline material of zeolitic nature (ITQ 20) and preparation process.; A microporous crystalline material of zeolitic nature, having the empirical formula x (M1 / n XO 2): y YO2: (1-y) SiO2, wherein x has a value less than 0.2; and it has a value less than 0.1; M is at least one inorganic cation of charge + n; X is at least one chemical element with oxidation state +3, preferably selected from Al, Ga, B, Cr, Fe; and Y is at least one chemical element with oxidation state +4, preferably Ge, Ti, Sn, V.; This material is obtainable by a process comprising: preparing a laminar precursor, crystallized from a reaction mixture; subjecting the precursor to swell in a solution to obtain a swollen laminar washing and dried to obtain a swollen solid material; subjecting the solid to obtain a delaminated delaminated material for suspension; separating the delaminated material and remove organic residues by cation exchange and / or calcining.
机译:微孔晶体沸石材料(ITQ-20)及其制备方法。具有沸石性质的微孔晶体材料(ITQ 20)及其制备方法。具有沸石性质的微孔晶体材料,其经验式为x(M1 / n XO 2):y YO2:(1-y)SiO2,其中x的值小于0.2;且其值小于0.1; M是至少一个电荷+ n的无机阳离子; X是至少一种具有+3氧化态的化学元素,优选选自Al,Ga,B,Cr,Fe; Y是至少一种氧化态为+4的化学元素,优选为Ge,Ti,Sn,V。该材料可通过以下方法获得:包括制备从反应混合物中结晶的层状前体;和使前体在溶液中溶胀以获得溶胀的层流洗涤液并干燥以获得溶胀的固体物质。使固体获得分层的分层材料以悬浮;分离分层材料,并通过阳离子交换和/或煅烧除去有机残留物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号