Process for the manufacture of a (co) methacrylate polymer which comprises carrying out the polymerization while supplying a monomer (mixture) containing at least 90% by weight in total of at least one methacrylate monomer and an initiator of the radical polymerization represented by formula (II) to a reactor, in which the concentration of the initiator and the polymerization temperature satisfy a ratio represented by equations (1) to (4) and the polymerization temperature is not less than 110 ° C and not exceeding 160 ° C; ln (A) 105, 4 ¿45126 / B (1) ln (A) 2545, 2 / B ¿15, 82 (2) ln (A) 225, 9 ¿102168, 8 / B (3) ln (A) 1300, 0 / B ¿15, 74 (4) in which A is an initiator concentration (a molar ratio of the initiator / monomer); B is a polymerization temperature (ºK); and ln is a symbol for a natural logarithm; wherein R is alkyl or fluoroalkyl.
机译:制备(共)甲基丙烯酸酯聚合物的方法,该方法包括进行聚合反应,同时提供一种单体(混合物),该单体(混合物)的总含量至少为90重量%,其中至少一种是甲基丙烯酸酯单体,并且由式(1)表示的自由基聚合反应的引发剂II)至反应器,其中引发剂的浓度和聚合温度满足由式(1)至(4)表示的比率,并且聚合温度不低于110℃且不超过160℃; ln(A)105,4¿45126 / B(1)ln(A)2545,2 / B¿15,82(2)ln(A)225,9¿102168,8 / B(3)ln(A) 1300,0 / B¿15,74(4)其中A是引发剂浓度(引发剂/单体的摩尔比); B为聚合温度(ºK); ln是自然对数的符号;其中R是烷基或氟代烷基。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号