A superalloy has a composition of, in weight percent, from about 16.0 percent to about 22.4 percent cobalt, from about 6.6 percent to about 14.3 percent chromium, from about 1.4 percent to about 3.5 percent tantalum, from about 1.9 percent to about 4.0 percent tungsten, from about 1.9 percent to about 3.9 percent molybdenum, from about 0.03 percent to about 0.10 percent zirconium, from about 0.9 percent to about 3.0 percent niobium, from about 2.4 percent to about 4.6 percent titanium, from about 2.6 percent to about 4.8 percent aluminum, from 0 to about 2.5 percent rhenium, from about 0.02 percent to about 0.10 percent carbon, from about 0.02 percent to about 0.10 percent boron, balance nickel and minor amounts of impurities. The superalloy is advantageously utilized in aircraft gas turbine disks.
机译:超级合金的成分为重量百分比为约16.0%至约22.4%的钴,约6.6%至约14.3%的铬,约1.4%至约3.5%的钽,约1.9%至约4.0%的钨钼:约1.9%至约3.9%,锆约0.03%至约0.10%,铌约0.9%至约3.0%,钛约2.4%至约4.6%,铝约2.6%至约4.8%含量为0至约2.5%,碳为约0.02%至约0.10%,硼为约0.02%至约0.10%,平衡了镍和少量杂质。超级合金有利地用于飞机燃气涡轮盘中。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号