PROCESS FOR PREPARING ENVIRONMENTALLY STABLE PRODUCTS BY THE REMEDIATION OF CONTAMINATED SEDIMENTS AND SOILS

机译:通过修复污染的泥沙和土壤来制备环境稳定产品的过程

摘要

This invention relates to thermo-chemical remediation and decontamination of sediments and soils contaminated with organic contaminants as well as inorganic materials with subsequent beneficial reuse. Novel environmentally stable products of commercial value are produced when certain additives such as calcium and metal oxides are mixed with the contaminated materials. In the process, the mixture is heated to 1150 DEG C. DIFFERENCE 1500 DEG C. to produce a molten reaction product with at least part of an excess amount of oxygen mixture or air is continuously bubbled through the melt in order to provide mixing and achieve high thermal destruction and removal efficiencies of the organic contaminants. The melt is then quickly quenched in moist air, steam, or water to avoid the transformation of the amorphous material into crystals. The inorganic contaminants such as chromium, nickel, zinc, etc. are incorporated and completely immobilized within the amorphous silicate network. The amorphous material can be pulverized to yield a powder which evinces cementitious properties either by reaction with alkali solution or by blending it with other materials to produce blended cements. The compressive strengths of the concretes made from the powder of the subject invention and blends thereof are comparable to, or greater than the ASTM requirements for general purpose concrete applications. The powder of the subject invention, blended cements, and concrete/mortar derived therefrom also easily pass the EPA TCLP leach test to achieve environmental acceptability.
机译:本发明涉及对被有机污染物以及无机材料污染的沉积物和土壤进行热化学修复和去污,以及随后的有益再利用。当某些添加剂(例如钙和金属氧化物)与被污染的材料混合时,会生产出具有商业价值的新型环境稳定产品。在此过程中,将混合物加热到1150℃。在1500℃下产生至少有一部分过量氧气混合物的熔融反应产物,或者将空气连续鼓泡通过熔体以提供混合并达到有机污染物的热破坏和清除效率高。然后将熔体在潮湿的空气,蒸汽或水中快速淬火,以避免非晶态材料转变为晶体。无机污染物如铬,镍,锌等被掺入并完全固定在非晶硅酸盐网络中。可以将无定形材料粉碎成粉末,该粉末通过与碱溶液反应或将其与其他材料混合以生产混合的水泥而具有胶凝性能。由本发明的粉末及其共混物制成的混凝土的抗压强度可与通用混凝土应用的ASTM要求相媲美或更高。本发明的粉末,混合的水泥以及由其衍生的混凝土/砂浆也容易通过EPA TCLP浸出试验,以达到环境可接受性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号