METHOD OF PRODUCTION OF COMPOSITION OF BUTADIENE-STYRENE BLOCK COPOLYMERS AND BUTADIENE-STYRENE BLOCK COPOLYMER COMPOSITION PRODUCED BY THIS METHOD

机译:制备丁二烯-苯乙烯嵌段共聚物的组成的方法和用该方法生产的丁二烯-苯乙烯嵌段共聚物的组成

摘要

FIELD: production of block copolymer compositions.;SUBSTANCE: method of production of butadiene-styrene composition of block copolymers (AB)nX having average weight molecular mass of 140·103 to 300·103 and polydispesivity of 1.20-1.50 and A1B1 having average weight molecular mass of 50·103-150·103 and polydispersivity of 1.20-1.40 (where A, A1 are polystyrene blocks, B, B1 are polybutadiene blocks. X is fragment of combining agent, n≥2, mass ratio of blocks A:B and A1:B1=(20-35):(80:65)% consists in successive polymerization of styrene and butadiene in medium of hydrocarbon solvent in presence of lithium organic initiating agent followed by stabilization and mixing of block copolymers without separation from solutions after polymerization at mass ratio of (AB)nX:A1B1= 1 : (0.06-0.15); flows of solutions of block copolymers are directed to averager through flow-type static mixer at rate of flows of block copolymer : antioxidant ≥ 1600:8.0 kg/h and mass ratio of block copolymer : antioxidant = 1: (0.005-0.0075); mixing in averager is continued for at least an hour at temperature not below 40 C and composition of block copolymers is separated by aqueous degassing method. Additionally, petroleum or mineral oil may be introduced in the amount of 5-8 parts by mass per 100 parts by mass of block copolymer composition at flow rate of block copolymer : oil ≥ 1600:800 kg/h.;EFFECT: enhanced heat resistance; increased productivity; improved technological properties of block copolymers.;4 cl, 4 tbl, 14 ex
机译:领域:嵌段共聚物组合物的生产;物质:平均分子量为140·10 3 n X的丁二烯-苯乙烯组合物的生产方法>至300·10 3 ,多分散度为1.20-1.50,平均分子量为50·10 的A 1 B 1 3 -150·10 3 和多分散性为1.20-1.40(其中A,A 1 是聚苯乙烯嵌段,B,B 1 是聚丁二烯嵌段。X是结合剂的片段n≥ 2,嵌段A:B和A 1 :B 1 =(20-35)的质量比: (80:65)%在于苯乙烯和丁二烯在烃溶剂介质中,在锂有机引发剂的存在下连续聚合,然后在聚合后以(AB)的质量比稳定和混合嵌段共聚物而不会从溶液中分离出来。 n X:A 1 B 1 = 1:(0.06-0.15);嵌段共聚物的溶液流动剧烈通过流动型静态混合器以嵌段共聚物的流量进入平均器:抗氧化剂≥ 1600:8.0kg / h和嵌段共聚物:抗氧化剂的质量比= 1:(0.005-0.0075);在不低于40℃的温度下,在均化器中继续混合至少一个小时,并通过含水脱气方法分离出嵌段共聚物的组成。另外,相对于每100质量份的嵌段共聚物组合物,可以以嵌段共聚物:油的流量引入5〜8质量份的石油或矿物油。 1600:800 kg / h。效果:增强的耐热性;提高生产力;改进了嵌段共聚物的技术性能。; 4 cl,4 tbl,14 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号