PPROBLEM TO BE SOLVED: To provide a reclaimed resin composition produced by melting and kneading a ground material of a molded product which contains a rubbery polymer and may contain an inorganic filler together with a virgin thermoplastic resin and a virgin inorganic filler, and capable of giving good processability, such as tap strength, and good mechanical characteristics, such as weld strength, to a reclaimed molded product. PSOLUTION: This reclaimed resin composition is produced by melting and kneading the ground material (A component) of the thermoplastic resin composition molded product which contains the rubbery polymer (A-1 component) in an amount of 2-10 wt% based on 100 wt% of the molded product and the inorganic filler (A-2 component) in an amount of 0-15 wt% together with the virgin thermoplastic resin (B component) and the virgin inorganic filler (C component), so as to produce the reclaimed resin composition (D component), wherein the rubbery polymer (D-1 component) is contained in an amount of 0.1-2 wt% based on 100 wt% of the reclaimed resin composition and the inorganic filler (D-2 component) is contained in an amount of 15-50 wt% based on the same. PCOPYRIGHT: (C)2005,JPO&NCIPI
机译:

要解决的问题:提供通过将包含橡胶状聚合物并且可以包含无机填料以及原始热塑性树脂和原始无机填料的模制产品的研磨材料熔融并捏合而制备的再生树脂组合物,以及能够对回收的成型产品赋予良好的加工性能(例如,敲击强度)和良好的机械特性(例如,焊接强度)。

溶液:该再生树脂组合物是通过熔融和捏合含有2-10重量%的橡胶状聚合物(A-1成分)的热塑性树脂组合物成型品的研磨材料(A成分)而制得的。相对于原始热塑性树脂(B组分)和原始无机填料(C组分),以100%(重量)的模塑产品和无机填料(A-2组分)的含量为0-15 wt%,制备再生树脂组合物(D组分),其中基于100wt%的再生树脂组合物和无机填料(D-2组分),橡胶状聚合物(D-1组分)的含量为0.1-2wt%。 )的含量基于该含量为15-50wt%。

版权:(C)2005,JPO&NCIPI

著录项

  • 公开/公告号JP2004323825A

    专利类型

  • 公开/公告日2004-11-18

    原文格式PDF

  • 申请/专利权人 TEIJIN CHEM LTD;

    申请/专利号JP20030397034

  • 发明设计人 TAKAGI MAKOTO;KIKUCHI SEIJI;

    申请日2003-11-27

  • 分类号C08L69/00;C08K3/34;C08K7/06;C08K7/14;

  • 国家 JP

  • 入库时间 2022-08-21 22:34:55

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号