摘要

PPROBLEM TO BE SOLVED: To provide a pelletizer capable of obtaining low-cost ground material with a small number of processes by using coal ash as main raw material. PSOLUTION: An agitation device 10 is provided with two rotation shafts 12 which are arranged parallel in an agitation tank 11 and rotate in reverse directions to each other, arms 13 disposed on the rotation shafts 12, a first blade 14 which is disposed on the top end of the arm 13a, pushes object material to be agitated against the inner wall 11a and grinds the same and a second blade 15 which is disposed on the top end of the arm 13b and scrapes the object material to be agitated attached to the inner wall 11a. By using the agitation device 10, object material to be treated such as coal ash and fused slag and object material to be granulated including hydraulic inorganic material such as cement are agitated, coal ash and cement are mixed, thereafter, water is added, at the same time, the rotation speed of two rotation shafts is elevated, the agitation is stopped after an elapse of a prescribed time and the granular ground material is obtained. Cement is preferably included in the range of 3 to 30 pts.wt. for coal ash 100 pts.wt. and water is suitably added to the mixture of coal ash and cement in the range of 6 to 30 pts.wt. PCOPYRIGHT: (C)2005,JPO&NCIPI
机译:

要解决的问题:提供一种造粒机,其能够以煤灰为主要原料,以较少的工序获得低成本的地面物料。解决方案:搅拌装置10设置有两个旋转轴12,其在搅拌槽11中平行布置并且彼此反向旋转;臂13布置在旋转轴12上;第一叶片14,其布置在第一旋转叶片12上。在臂13a的顶端上,将待搅拌的目标材料推向内壁11a并对其进行研磨,并且第二刀片15布置在臂13b的顶端上并刮擦待搅拌的目标材料。内壁11a。通过使用搅拌装置10,搅拌煤灰和熔渣等被处理物以及水泥等水硬性无机物等造粒物,将煤灰和水泥混合后,在水处添加水。同时,提高两个旋转轴的旋转速度,经过规定时间后停止搅拌,得到粒状粉碎材料。水泥优选包括在3至30pts.wt的范围内。煤灰100 pts.wt.将水适当地以6至30pts.wt的范围添加到煤灰和水泥的混合物中。

版权:(C)2005,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号