首页> 外国专利> At centrifugal casting equipment casting the ductile

At centrifugal casting equipment casting the ductile

机译:在离心铸造设备上铸造球墨铸铁

摘要

PROBLEM TO BE SOLVED: To provide a ductile cast iron pipe having a small content of impurities such as P, Cu and Cr and excellent mechanical properties such as elongation or impact value and a manufacturing method therefor.;SOLUTION: The ductile cast iron pipe is obtained by casting blast furnace molten iron applied with desulfurization and dephosphorization by a centrifugal casting equipment and contains ≤0.02 mass% P, ≤0.03 mass% Cu, and ≤0.03 mass% Cr. The manufacturing method for the ductile cast iron is performed by applying desulfurization and dephosphorization to the molten iron tapped from the blast furnace, next adding a graphite spherodizing agent to the molten iron, and after that, casting the molten iron by the centrifugal casting equipment to form a cast iron pipe.;COPYRIGHT: (C)2002,JPO
机译:要解决的问题:提供一种球墨铸铁管及其制造方法。该球墨铸铁管具有少量的诸如P,Cu和Cr的杂质,并且具有优异的机械性能,例如伸长率或冲击值。通过使用离心铸造设备对施加了脱硫和脱磷作用的高炉铁水进行浇铸而获得的合金,其含有≤0.02质量%的P,≤0.03质量%的Cu和≤0.03质量%的Cr。球墨铸铁的制造方法是通过对从高炉抽出的铁水进行脱硫和脱磷,然后向铁水中添加石墨球化剂,然后,通过离心铸造设备将铁水铸造至铸铁管。;版权所有:(C)2002,日本特许厅

著录项

  • 公开/公告号JP3672832B2

    专利类型

  • 公开/公告日2005-07-20

    原文格式PDF

  • 申请/专利权人 日本鋳鉄管株式会社;

    申请/专利号JP20010063236

  • 发明设计人 川上 正弘;石川 勝;

    申请日2001-03-07

  • 分类号C22C37/04;B22D13/02;C21C1/02;C21C1/10;C21C7/064;C21D5/00;C22C37/06;

  • 国家 JP

  • 入库时间 2022-08-21 22:28:45

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号